3/2/16       
Matt M

We build mostly euro boxes, but when we do build a face frame cabinet, it's almost always a large beast (such as bookshelves with arched tops, etc).

It's enough that I'm considering buying a vertical face frame assembly table with the pneumatic clamps on a roller gantry.

I've used them before at a previous shop, but that was 10 years ago and I have no idea the manufacturer.

I see offerings for 4X8 tables from Kreg, Castle, and WoodTek. Kreg is around $3,400. Not sure of the price on Castle or Woodtek.

Looking for opinions. I definitely want a 4X8, with a good clamping system. Pneumatic clamps are nice, but I'm ok with manual (lever style) clamps.

Thanks,

Matt

3/2/16       #2: Face frame assembly table w/ clamps ...
Bruce H

I don't think it would be worth the space it would take up for an occasional use. I use a pair of vise grips and a flat bench or piece of melamine. Not perfect but I am also an euro shop and don't do it often.

3/2/16       #3: Face frame assembly table w/ clamps ...
Matt M

Space is actually the very reason we want one. We do them often enough, and large enough, that it occupies our raw wood assembly table more than we prefer.

I have exactly what you are talking about already.

3/2/16       #4: Face frame assembly table w/ clamps ...
Bob

I have the Kreg 4X8 table with pneumatic clamps and have been very satisfied with it. Very seldom have I needed anything larger. I probably have been using it for 12 -15 years with no problems. I did not like the coiled hose on the screw gun so I replaced it with a short straight air line. I also added a shelf just below the table to hold screws and drawer opening spacers.

3/2/16       #5: Face frame assembly table w/ clamps ...
Peter Rawlings

Matt, don't know where you are or if bigger would fit in the space you have, but I picked up a used Ritter 5x12 for $1000 a few years ago and I've seen 'em for less since.

Parts might be a concern going forward though, I think Ritter closed their doors and their clamping rams were proprietary if I'm not mistaken.

3/2/16       #6: Face frame assembly table w/ clamps ...
Jim

I have a castle 4x8. Castle makes an extension for wider than 4' face frame.

3/5/16       #7: Face frame assembly table w/ clamps ...
Cabmaker

We have recently put a lot of resources into face frame manufacturing. Most of our work is flush inset and a lot of that uses fully mortised butt hinges. This is a lot easier to do if the face frames are really square.

Our wide belt sander is 42 inches wide but about 20% of the frames we build seem to not fit within that constraint. Rather than have some of the frames hand sanded and some of them wide belted we developed systems to make it so that no face frames had to be wide belted after being pocket screwed. We do have to have to kiss the joint with a random orbital sander to deal with grain raise from wiping glue but this is way better than also having to sand the cross grain marks off the frame. It's also easier for inexperienced people to be successful.

Our protocol is to polish sand the exposed face on the wide belt then, with this face oriented down, we run the stick through a dedicated planer that always produces 24mm thickness. This planer has a spiral head so produces a fairly clean face. With this system we know that every part is the same thickness every time.

The cross grain dimension is wide belted to thickness as needed. This is the weakest part of our system so far but we can usually absorb minor variation at this step. We have an idle shaper that will eventually be set up with a fence away system for controlling the cross grain width.

After the parts have been chopped and drilled for pocket screws the sticks go onto the face frame clamp. We have a Ritter that we bought from one of the other guys on this forum. The Ritter beam came with three clamps but we only use the bottom one. The other two are actually in the way. Eventually we will will pull them off and use them in some other process.

The Ritter Clamp easel is made out of steel with a grid of holes to position. This seemed to work but any excess glue that was left on the table seemed to weld itself to the steel.

These lumps of glue, albeit small, were the root cause of needing to wide belt the frame after assembly. Our solution was lay a piece of plastic laminate onto the table and glue a strip of laminate to the three fences. The plastic laminate makes it really easy to clean up glue after the frame is made.

We replaced the air pistons that push sideways with magswitch clamps. These have about 150lbs pull and reach right through the plastic laminate like it wasn't there. The clamps hold the parts in correct alignment and the endgrain always lines up perfectly with the side grain.

The extra attention we pay at this phase makes door fitting quite a bit simpler as well. We added a bunch of new clamps recently to facilitate building these frames in a bucket brigade. An experienced person sets up the parts while an inexperienced person drives the screws home and mops up the glue.

This bucket brigade approach has helped us add inexperienced people to respond to the current surge of customers. The new people become useful on their first day.


View higher quality, full size image (692 X 896)

3/7/16       #8: Face frame assembly table w/ clamps ...
Matt M

Cabmaker, fantastic info and I appreciate that you took the time to respond in such detail.

3/10/16       #9: Face frame assembly table w/ clamps ...
KAP

Assuming your parts are already pre-planed to size, you don't need a $3-$4K table setup...

All you need is a right angle setup like below (table is laminate for flat surface and easy glue squeeze-out clean-up)... hand pressure is all that's needed...

Best of luck... 8^)


View higher quality, full size image (687 X 422)

3/14/16       #10: Face frame assembly table w/ clamps ...
Matt M

We do pre-plane. Your corner squares are a simple thing, I'll give those a try. Not something I ever thought of to be honest with you, looks like a great idea.

We would have to set it up vertically like the pre-fab tables, but I can't see why that wouldn't work.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)