I've been using prefinished import ply for several years with pretty good results. Every once in a while I'll run on to some that will de-laminate, here lately I've run on to some that the veneer is just not glued well. My sales rep sent me a sheet today of domestic, Columbia I think. Judging from the one sheet it looks like the finish is some better, it's maple instead of birch, 3 larger core sheets instead of several thinner sheets. Looks like the 1/2" runs about $15 more and about $20 more for the 3/4". Question is, is the domestic worth the extra money? How consistent is the quality? Any other pros and cons that I'm not thinking of?

5/11/16       #3: Prefinished ply: import vs. domesti ...
Dustin orth

Website: http://customwoodmontrose.com

I have found that not having to check every sheet for a delamination or garbage finish is worth the extra money. Not to mention my main supplier doesn't even carry the import stuff. To many rejects when they did. My 2 cents.

5/11/16       #4: Prefinished ply: import vs. domesti ...
John B Member

Website: http://woodmanseewoodwrights.com

I agree with Dustin. It's bad enough dealing with sorting sheets that are bad, but even worse is when you use one that looks OK, then after the cabinet is built it starts to delaminate. Not worth the small savings, at least for me, as most jobs are higher end.

5/11/16       #5: Prefinished ply: import vs. domesti ...
JeffD

I won't use the import stuff, heard too many complaints over the years. Also hard to justify to my client they spend more money for custom built cabinetry and then go and buy the cheapest stuff available to build it.

I did recently try a less expensive version of domestic, (supposedly), pre-finished maple from one supplier who couldn't tell me why it was cheaper. They insisted it looked the same and a lot of shops were using it. Didn't look the same to me and won't be using that again either.

good luck,
JeffD

5/11/16       #6: Prefinished ply: import vs. domesti ...
Mike Fuson

I got the actual prices today.
1/2"-$28 vs. $48
3/4"-$38 vs. $78
That's quite a price difference, I guess it's all in how you look at it. Probably would average around $500 extra for the average kitchen. On the other hand, I did get a few sheets of the import in yesterday and there was no delamination issues with what I cut so far. Thanks for the responses.

5/11/16       #7: Prefinished ply: import vs. domesti ...
Hen Bob Member

I second JeffD with the less expensive domestic stuff. I tried a dozen or so sheets and it did not look consistent like I'm used too.

Keep shopping around Mike, I pay $58-$61 for 3/4, $44-$46 for 1/2. One side finished

5/11/16       #8: Prefinished ply: import vs. domesti ...
James sarver

My local supplier has import maple i really like it alot over birch most of our suppliers carry fir core over popular core in there domestic ply

5/18/16       #9: Prefinished ply: import vs. domesti ...
Gary

I would look at Garnica Spanish company it weights 30 less than domestic poplar cores. Their poplar cores are plantation grown no dark mineral streak telegraphing thru veneers there is little to no voids and I find this plywood very stable and the thickness consistency is is about a B+ they only down side I found but over cam was screws stripping out easier so we drill 4mm holes for hardware screws problem solved.

I was a big Columbia product guy are years had all kinds of issues the new MPX cores to inconsistent is thickness for CNC. They finally have a seamless outer band of poplar before they fixed that I can't count how many ends I replaced I was using there Kcore calibration on that was about a B I had my fair share of delamination problems as well

I used States plywood for a short time there fir core doesn't work up here in New England but I have to say the calibration is a A+

In my area all the suppliers want to carry Garnica that says something about the product. I hope some day soon Columbia listens to all the cries for better cabiration and telegraphing problems I still like the company but losing faith that they will come up with something soon

5/19/16       #10: Prefinished ply: import vs. domesti ...
Mark Elliott Member

I too dropped Columbia for Garnica and have never been happier.

It's a great product and I highly recommend it.

I too hope Columbia wakes up and gets their act together. There should be no need to have a better made plywood shipped from Spain to here at a lower cost.

Mark


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)