Website: http://www.jescopr.com

I custom build contemporary frame-less cabinets. I currently use what's left of a minimax me15 hot air edgebander. I would love pre mill, scraper and buffer. I wasn't able to attend the IWF Atlanta. I've been looking at cehisa mykro p plus, Felder G330, Minimax ME 25 and 28. Any suggestions and experience advice is welcome. Thanks!
https://www.felder-group.com/us-us/products/edgebanders/edgebander-g-330.html
https://www.scmgroup.com/en_US/scmwood/products/joinery-machines.c884/single-sided
-automatic-edge-banders.885/minimax-me-25.650
http://www.cehisa.es/en/edgebander/14-edgeband-mykro-p-plus-cehisa.html

9/9/18       #2: in the market for edgebander Felder ...
Jeff

It is my experience with woodworking equipment, that you buy a brand that you can get good service relatively easy. It is only a matter of time before you will have an issue and if the machine is sitting there and you are waiting for parts and service, it is a huge issue.
I am not sure how big of an operation you have, but an edgebander should only be a 1 or 2 person machine, as soon as you start having everyone run it, well lets just say your in trouble.
I personally wouldn't buy anything Cehisa or Felder as I am not a fan of their equipment. I have never used a minimax edgebander, but they are made by SCM and they make excellent edgebanders.
If you are looking to buy used there are a lot of the SCM edgebanders on the market, you can pick up a 201 for really cheap, I would of course get it inspected by a tech before purchasing, another machine that i would buy used is a Brandt, something like a 340, very good machines with scraping, solid wood capabilities, 3 mm round over for 3 mm edging.
A new glue pot on these edgebanders is ballpark 3 grand, so make sure you get them inspected if buying used.

9/9/18       #3: in the market for edgebander Felder ...
David Shumway  Member

Website: http://www.jescopr.com

Thanks for the advice. Being able to service the machine when it breaks down (they always do) is important. I have two friends that have the ceshia edgebander they bought from Adwood and they seem quite pleased. I've read they are built like a tank and Adwood does a good job of providing support. I don't know anyone locally who owns Felder. I have 2 scmi machines and they are quite solid.

9/9/18       #4: in the market for edgebander Felder ...
Gary Balcom

David,

I would take an honest look at Cehisa. We are a production shop, and run a Brandt as our main bander. I bought a used Cehisa EB-7 for the short ends of one particular phased project. We've run over 50,000 edges through that little machine with few complaints.

9/9/18       #5: in the market for edgebander Felder ...
Mikel Sinclair Member

I own the Felder G360. I believe Felder makes some very solid machinery; their edge bander is NOT one of them. They are really quite new to banding equipment and are a long way behind the leaders.

9/9/18       #6: in the market for edgebander Felder ...
ANDREW KREUTTER Member

Website: Aka Enterprises

I shared this in another post
We just installed a new 6.5 VantEdge Bander from Ed Moran and VTM. I looked at all the Banders at IWF. everything remotely close to what we purchased from Ed was over $20,000 more than what we paid. Anyone is welcome to give me a call or Stop out to my shop to see the Bander in action. We are doing high gloss doors and residential and commercial work. Send me a text to 716 474 4579. We are in Wyoming NY 14591

Ps Ed sold me the machine and came out to my shop himself and spent 2 days getting us set up and trained on the machine. Ed designd the machine, sold me the machine, and he is the tech that installed the machine and addresed every issue and question I had. We ran actual jobs on the machine as we dialed it in. I am a happy customer!

Ed Moran had helped me repair our old Edgebander in the past. Ed is a mechanical and electrical technician. I was a bit skeptical of a bander that was full of proprietary parts from China. We made our decision after many conversations, and after looking at many edgebanders.
The electronics used in our Vantedge bander are non proprietary and available here in the USA. The finish and quality are equal or better than some of the actual European machines we looked at. Ed designed these machines around the experience he has gained working on edgebanders over the years. Ed was physically at the factory and communicating with me, via pictures and video while our machine was built. I am thinking I will start a new post to communicate our good and bad experiences we may have as we use this machine. We band alot of material every day at our shop. I will let everyone know how this works out. We have 1 week of full production on the machine now.


View higher quality, full size image (1440 X 1080)


View higher quality, full size image (1440 X 1080)

9/15/18       #7: in the market for edgebander Felder ...
Harold morantz

Website: http://morantzcabinets.com

I owned a Cehisa for 14 years and it was a good machine that was very user friendly. The shop that bought it from me is also very happy with it. We also build modern cabinetry frameless and our thickest banding is 1mm. I bought a used Brandt with premill, corner rounding and preheat glue hopper that turned out to be a major mistake as I trusted the machine company I bought it from and it had not been used in over a year and needed major work. I paid 20k which included a new gluepot, but all the knives were for 3mm and many parts needed replacing and the labor for. The techs and parts cost me over 15k. The corner rounding was not repaired as it would cost another few thousand and with 1mm pvc tape, is not really needed. I also had to get a much bigger dust collector to handle this machine. It is working great now and we have refined the programs that any of my 6 guys can use it, but it is really big and overkill for doing 1mm or even 2mm work. Probably could have bought a new bander that would have more electronic line control and less time wasted setting it up and dealing with all the down time till we got it where it did what we required. In the mean time I have spoken to the shop that bought my used Cehisa and it has made enough money for them to go into CNC.
Lessons learned: have used machinery inspected and don’t trust used machinery sellers, be realistic about what your actual needs are instead of emotionally decision to have a large impressive bander, go to shows or other shops that are doing the same work as you.
Harold

9/15/18       #8: in the market for edgebander Felder ...
David Shumway  Member

Website: http://www.jescopr.com

Thanks for the info.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)