pressure pot set up -- 1 -- 
10/9

I am looking to get into a on site water bourne paint system. I am set up now with a Makita 2.5 hp 4.2 gallon 4.2cfm compressor mounted on a cart to run my Kremlin 10-14 pump. I use this set up to spray Clawlock and Krystol with great results. I can feel the water base pressure coming and want to get on board. Can i just switch to water bourne with my set up? Been reading trouble with micro bubbles with the kremlin and water bourne. Some have stated they get better results with a pressure pot with water bourne. My Makita keeps up not to bad with the kremlin but would it have enough umhp to feed a pressure pot?
Jeff
10/9 #2: pressure pot set up ...

For any kind of real production your compressor is too small. There are a few guns on the market that are advertised to work with as little as 4cfm but even at that your compressor would be going all the time to keep up with any continuous spraying and with such a small tank you won't be able to build up much of any reserve when your not spraying.
That is the down side of the pot/gun set-up when compared to a AAA, it uses a lot more air.
I'm one of the ones who prefers the pot/gun to the pump and I've outfitted myself with a number of set-ups for clears, pigmented and stain but most of my stuff uses at least 10cfm and some 15cfm+. I have a 5 hp, 17cfm, 80 gallon tank Curtis in the shop that powers it all no problem. But you can't haul a 500lb. 3 phase compressor to the job site, so for on site work I use a 4 stage turbine and either a 2 gallon or 2 quart pot for the WB's, I just bring along a little compressor to push the material from the pot to the gun...works great.
10/11 #3: pressure pot set up ...

I have a turbine and a 2quart pot but found it very bulky to get in and around inside cabnets and making sure as to not let the pot fall over.I did make it work but it was very slow and and a pain to deal with. I love my kremlin and and solvent base products,just have to start the re-learn curve with water bourne.
10/11 #4: pressure pot set up ...

I made a simple base to hold my 2 quart pot, a box with a hole to fit the pot screwed to a larger plywood square.
10/12 #5: pressure pot set up ...

Thanks for the replys. I find that the hose from the pot to the gun is to short-3-4 feet. I have to have one hand holding the pot at all times. Plus the fact of the larger hoses attached to the gun make it much more difficult to twist and turn the gun to spray with.I have also used a gravity feed gone and noticed alot more over spray than the Kremlin. Never used a pot gun before so have comparison. I like the idea of having the paint set in one spot then just move around the site with gun and hose only. I put on a 40 foot hose on my Kremlin so i can set it in the middle of most hall ways and it allows me to spray the kitchen cabnets ,move to the hallway bathroom cabnets then to the master bed room for the ensuite bath room.This works very well with my solvent materials so would like to make water bourne work much the same way.
10/12 #6: pressure pot set up ...

I'm guessing you work mostly onsite, so portability is the primary concern. Of course an airless is the ultimate in portability; powerful, light weight, 110 volt powered and one fluid line and 100' of fluid line is no problem so the pump can be a long way from the work...the down side is; if you're not use to the speed problems can arise in a hurry (runs, sags and over-spray).
A turbine unit can slow things down enough and if you have powerful enough unit you can get beautiful results with them but the lines are bulky, they are loud, they get hot and need a break every now and then, they work best with fairly short air lines (I use 25' on mine) so chances are you'll be moving them around but should still be placed as far away from the work as you can so you don't clog up the air filters. I use one (Graco 9000) for on site but onsite work but average only one day a month spraying with it, if I did much more than that I'd be looking for a different set-up.
Both Binks and CAT make portable compressor powered pot/gun set-ups that run off of 110. They look to come complete except for oil/water filters. They are spendy; the CAT system is advertised at $1,700 + (you could get a CAT WB AAA for that) The Cat is heavy at 150lbs. +, Binks says around 70lbs. for theirs. I'm guessing they're loud and they only come with 25' of air/fluid line, so you'd be moving it around a bit. If I sprayed WB's on site a lot I'd consider this as a option.
The last possibility would be a AAA, I've used my 10:1 for WB's in the past and got good results just not as good or as consistently good as the pot/gun. I know CAT has slightly altered their 14:1 to make it more WB friendly. I have yet to use or seen the results of one in use but if it works as advertised; this might be what you're looking for...maybe someone with experience with one will chime in hear.
10/12 #7: pressure pot set up ...

I have tried spraying trim and door jambs with latex and a airless and found it was not what i wanted to continue useing. I have sprayed hundreds of gallons of latex thinned slightly out of my Kremlin portable outfit with excellent results. I always used a color product so was wandering why there was this micro bubbling in the water bourne products? I haven't sprayed any so was hoping to get some feed back on users experience and suggestions .
10/12 #8: pressure pot set up ...

Why not just use the Kremlin? Switch to an xx-052 waterborne tip and spray away. (put whatever size tip you prefer into the XX, 06 or 09)
10/12 #9: pressure pot set up ...

I am using a 06-114 so what would be the tip # i would need to order. I would like to continue using the Kremlin set up as long as the water bourne finish works .I have access to MLC products.
10/12 #10: pressure pot set up ...

"I am using a 06-114"
For an extra fine finish tip with the same size fan you would order an 06-112. Your Kremlin dealer should be able to help you.
This shows all the tips
10/13 #11: pressure pot set up ...

Thank you everyone for the replys . I will start with a new tip and pick up a gallon of white and a gallon of clear . 99% of my work is refinishing on unknown coatings. I use Vinyl sealer for my base with solvent finish what will i need for water bourne?
1 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|