Kem Aqua Plus -- 0 -- 
5/15

I haven't run into this before, but on a recent kitchen, (last fall), I sprayed pigmented Kem Aqua Plus over their recommended sealer. I just had a callback and there appears to be a couple small spots that flaked off, maybe 1/2 - 3/4" long at the beaded face frame area. I don't know if sanding too fine might have been an issue or bad primer or what. Wood is hard maple sanded to 220. Anyone had issues with this finish bonding well? Bare wood shows so the primer seems to not have hung on. It also doesn't appear to be a customer damage thing.
5/15 #2: Kem Aqua Plus ...

I think 220 is too fine for most finishes these days. I sand to 150 for pigmented finishes.
I would check the spec sheet but I am quite sure that would be the recommendation.
5/15 #3: Kem Aqua Plus ...

Pretty sure the recommended sanding for waterborne is 220.
I don't have much experience with waterborne because I feel it isn't quite there yet.
5/15 #4: Kem Aqua Plus ...

Like Leo, I use mostly solvent base so I could be off base on the waterborne finish.
This is from the Clawlock spec sheet.
"For best adhesion, finish sanding on wood, should be done using a maximum of 150 grit paper."
Always best to check the manufactures application instructions but I think with a primer coat going on I would not go that fine.
5/16 #5: Kem Aqua Plus ...

"Wood Finishing System
1. Primer—apply Sher-Wood Kem Aqua
Plus Surfacer at 4-5 mils wet. Air dry
thoroughly. Sand with 240 grit sand-
paper. A second coat of primer may be
applied for improved holdout. Sand
between primer coats and before top-
coat.
2. Topcoat—apply Sher-Wood Kem Aqua
Plus White at 3-4 mils wet. A second
coat may be applied. Sand with 240
grit sandpaper between coats.
3. A coat of Kem Aqua Plus Clears can
be used a final coat for added perform-
ance properties.
4. Dry—allow overnight drying before
stacking or packing
5. Maximum dry film thickness of the
system should not exceed 4 mils. "
5/16 #6: Kem Aqua Plus ...

Thanks for the input guys. I think I followed the correct procedures from what I have read on the Kem Aqua site. It really seems as if it's a primer issue as where the finish is off it's right down to bare wood. I've used BIN's alcohol based primer before under other waterbourne finishes with no problem but in this case used SW primer they recommended.
5/16 #7: Kem Aqua Plus ...

imo sanding maple to 220 grit is way to fine for raw wood sanding for waterborne or solvent coatings. If an operator by machine, random orbit or by hand is over using their paper, then you have potential to be sanding to a final smoothness of 320+ aluminum oxide abrasives we typically sand with for raw wood are designed to dull their cutting points as it's abraded, thus leaving a finer finish when the abrasive has reached it's pinnacle. silicon carbide grain is designed to fracture under pressure always leaving a sharp cutting edge to the grain structure and that's why we use silicon carbide to sand sealer or finish... so it cuts well and leave a consistent depth of scratch. IMO for first initial coats on any species for maximum adhesion 150-180 grit is the maximum.....
5/16 #8: Kem Aqua Plus ...

I've used WB for almost 15yrs and I think 220 especially on hard maple is not the way to go. The possibility of burnishing is definitely in play.
You say it's on a beaded face frame? Not the doors? It's possible A. minor contamination before sealing. B. wood movement with moisture from normal kitchen usage. If your issue is near the sink or dishwasher(think steam) areas wood movement allowing moisture into and under the finish could be the culprit.
my2cts
good luck
5/16 #9: Kem Aqua Plus ...

What Leo referenced about 240 grit is for sanding after the primer, at least as I read it.
John
5/16 #10: Kem Aqua Plus ...

i recently did a project in maple with the white kem aqua plus. sanded the maple to 120, primer (i used the shellac-based zinsser), two coats of kem-aqua white, 220 in between. came out good.
on my test piece, i sanded the primer and between coats with 150, and you could definitely see swirls through the final coat if you look with good light. not so with the 220.
good luck,
--- dz
5/16 #11: Kem Aqua Plus ...

My opinion differs; when using a WB primer on bare wood (something I avoid if at all possible) 220 grit white wood sanding should be fine all that h2o and possibly the water soluble solvents in the primer are still going to swell the wood which should give you plenty of profile for your primer to hold onto.
As to why you have some lifting/peeling; I'm guessing you're getting some moisture in behind your finish resulting in some swelling and shrinking. Kem-Aqua dries hard and has very little flex, it just takes a just a couple of swell/shrink cycles and it will start to pop.
5/16 #12: Kem Aqua Plus ...

Using the pigmented primers I don't see a downside to sanding the wood with 150. The primer fills well enough to hide any scratches in the wood. I would not use 150 to sand the primer I use 280 to 320 for that. We use one heavy coat of primer sanded back very well with a lighter coat on that scratch sanded before the topcoat.
Of course the peeling could be completely unrelated to the white wood sanding.
5/17 #13: Kem Aqua Plus ...

A question for those who use the WB primer and the BIN white alcohol primer. Do you get more grain rising with the WB to the point that it is not worth it?
5/17 #14: Kem Aqua Plus ...

Thanks again for all the info. I do think I may go to maybe 180 for my final sand of the bare maple next time. If there was a moisture issue in the wood it seems as if the failure would be between the more flexible primer and the finish coats but I'm not sure, just guessing. One spot was near a sink but the other is not. One issue I have noticed with sinks is the farmhouse sinks that are not wiped down after using them. Water on the top front edge runs down the face and right onto the cabinets, unlike a drop in with an overhanging countertop. Might be a long term issue for finishes there.
5/17 #15: Kem Aqua Plus ...

Most of my experience is with MLC products. Their Agualente primer(and the Polystar before it-17yrs ago) is one of my favorite products. It goes on thick while leveling out perfectly. The can feels like a bucket of sheetrock compound. It sands like auto primer. No grain raise.
I've used buckets of BIN as well. The BIN sands harder, clogs the paper, and raises the grain more. Its more like sanding sealer. Not as good a coverage because its so thin. It also clogs the tips frequently.
We frequently do primed only work. The customers often thin the cabinets are done, because we lay on a heavy coat of primer then lightly sand it with 240.
Our schedule for all products is 150 grit wood, primer, 240 grit, 1st topcoat, 320 grit, 2nd topcoat.
5/18 #16: Kem Aqua Plus ...

bare wood sanding = 150
between coats = 220
Primer needs the scratch pattern to promote adhesion (give it something to bite). Any primer worth a damn will contain enough solids to fill the measly 150 scratch.. if it doesnt, find a better primer.
5/18 #17: Kem Aqua Plus ...

"I think I followed the correct procedures from what I have read on the Kem Aqua site. It really seems as if it's a primer issue as where the finish is off it's right down to bare wood."
you have clearly not followed the correct procedure. If your primer is falling off the wood completely your preparation is to blame. you need to promote the adhesion, not polish the wood. I never sand substrate past 150 before primer. The only time ive ever had adhesion issues was when i worked for a company in my early years that prepped their maple to 220 before primer. We would often see finish flaking off to bare wood and the finishers would blame the primer.
When i began to have a much better understanding of the limitations of coatings and how to properly prepare bare wood i have had no issues. So you can go ahead and prep it to 180 if it makes you feel better, but may i ask you what you have to gain by sanding with a higher grit? I mean 150 would obviously level your surface and remove defects faster, and will also give a deeper scratch pattern/promote adhesion.
0 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|