P. Sapele and Qtd. Mahogany veneered top. The core is a resin honeycomb sandwich which allowed wire chase for power and data. The fun part was building a 9' x 9' press bag. I built a temporary bag out of 6 mil plastic sheeting. There were a few leak issues, but it pulled a good vacuum

The sapele was a bleed-through nightmare even with the Blocker added into the Unibond. It telegraphed the veneer tape in spots, so I used a few coats of thinned shellac to fill the pores, and violla, no more telegraphed veneer tape.