Birds Eye Maple and Black Walnut Chest

Listing #4176 Listed on: 08/03/2013 Company Name: Custom Woodworking by David Tully
Name: David Tully Member

Birds eye maple and black walnut blanket chest. The panels are glued up birds eye maple veneer that I did in shop. The top is 7/8 inch thick solid black walnut. The bottom of the inside is lined with cedar. I make all moldings in house so all the grain and color are well matched.

3 Photos
Social Media:
Viewer Comments:
Posted By:steve
Great job and beautiful timbers.

Add Your Comment:

*Enter the correct numbers into the field below:

Date of your Birth:

WalzCraft Original Saw