First dovetail infill plane

Listing #5106 Listed on: 10/18/2019 Name: kolwdwrkr Member

This is my first dovetailed infill plane. It is made with brass, a cheap steel sole, 01 tool steel blade, and wenge wood. I know it's not a sauer-steiner but maybe if I made 30 planes a year like he does I can get there. I'm excited to start another one. As always I welcome criticism, positive or negative.

6 Photos
Social Media:
Viewer Comments:
Posted By:D Brown
A thing of Beauty for sure, great work would love to have a look at the sole, thanks for sharing.
Posted By:Tom Gardiner
Overall a beautiful plane. One criticism I have is I think you should work a larger radius on the tote. We expect to see and feel a tote that allows you to wrap your hand around without corners.
Posted By:David R Sochar
How do you cut the dovetails on the sole and sides? What equipment is required? Milling Machine?