I'd like to achieve the grey, oxidized look on a finished piece of furniture using some sort of treatment - not the sun and the rain. Does anyone know the method for doing this?

Forum Responses
(Finishing Forum)
From Paul Snyder, forum technical advisor:
There are chemical treatments you can use to make the wood gray (e.g., tannic acid and iron sulfate), but it changes color when you apply a finish. If you have a piece of weathered wood, wet it with water and see how the color changes. That's what a finish does. To get around the problem, I use two coloring steps. First, I'll dye the wood a grey color to get the shimmering effect and grain definition it has on the wood. Then I'll seal the dye (which changes its color) and then use a grey pigmented toner over the sealer. The pigmented toner brings back the grey color.

Click here for full size image

From contributor A :
The samples were done with an acid stain made up of household vinegar, a couple of steel wood pads, and some old rusty nails. Allow the brew to cook and from time to time you can test the stain on your wood until you get the color you are looking for.
You can get many colors from this stain. I choose these 4 colors to make up the sample. Some finishers actually allow the stain to go black, and then reduce the color with clean vinegar.

Click here for full size image

The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor A:
If you are going with iron sulfate be patient. Several coats may be needed but the product is sustainable so there is no smell and it dries fast. Mixing the product over the recommended ratio can give it a greenish tint. Itís definitely the most natural look of all the methods we've tried. The vinegar method works great on lighter shades of hardwoods.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article