Today's
Sponsors:


Mereen-Johnson Machine Company

Merritt Woodwork

MFG in Honduras

Micro Fence

Microvellum

Middle Valley Lumber

Mikron Woodworking Machinery

Mill Outlet

Minimax

Mirror Reflections

MLS Machinery USA, Inc.

MLS Machinery

Modern Woodworking Magazine

Moldingknives.com

Monarch Machinery

Morbidelli

Moulder Services

Moulder Techniques

Mountainside Wood Products

Multicam, Inc.

NAP Gladu

Nebraska Tool

NEMI

New England Kiln Drying Association

NexGen

Hoffmann Machine Company

Holz Her U.S. Inc.

Howard S. Twichell Co.

Hvalsoe Sawmill Ltd.

ICA North America

Icy Straits Lumber

IDM

Impact Search and Placement

Indiana Hardwoods

Industrial Air Solutions

Integra Precision Grinding and Manufacturing

InTrading

Invicta Woodworking Machines

IpeDepot.com

irsauctions.com

Italpresse

J & G Machinery

J and J Barn Wood

J&P Machines

J. Gibson McIlvain Company

Jiffytops

JIT Hardware Supplies, Inc.

JMHsoftware.com

John G. Weber Co.

Joos USA Inc.

KCD Software

Kerber Farms and Mill

Keystone Wood Specialties

Keytrix Data Systems

Kiln-direct.com

Kleiberit Adhesives USA, Inc.

Kreg Tool Company

Kremlin

Lacy Cypress Inc.

Langelier Lumber Ltd.

Leadermac USA

Lewis Lumber Products

Lignomat

Logosol

Lumber Resources

Lumber Smith

M.L. Campbell

MACHINEKING.com

Macoser, Inc.

Mahros

Maine Timber Works

Maine Woods Company

Mann and Parker Lumber Co.

Martin Lumber

MARTIN Woodworking Machines Corp.

Mastercam - CNC Software

Matthews Mill

Maya Positioning Equipment




A Small Solar Kiln       Report and photos of a small, just-finished solar kiln. November 8, 2007

Question
First, want to say thanks to the contributors on this board that helped with all the information to build a solar kiln. Using two solar powered fans for circulation, you can see the collectors mounted inside to help keep them from getting damaged. Kiln is 4'x8' and the entire bottom half of the back is covered by two doors that open so I can load wood on a pallet with a Bobcat. Pallet size is 6'6"x30" and circulation seems good so far. First charge is red oak, 13% MC when it went in 3 weeks ago, about 9% now. Temperatures have been as high as 125 degrees, but we're now starting to get some warmer weather, so hoping for a few days above 130 degrees to make sure any bugs are dead. As you can see, the kiln is built on skids, so it can be moved with the Bobcat and loaded on a trailer. Only for hobby use, but wanted it self contained so that's why I went with the solar fans - they were about $180 each including the panels. Collector is two layers of clear, fiberglass panels. Total cost was about $900 here in N. VA. Thanks again to all who post and provide this great resource.


Click here for higher quality, full size image

Forum Responses
(Sawing and Drying Forum)
From contributor T:
Nice job. Thanks for posting the picture so we can see it. What are you going to load it with next?



From the original questioner:
I have enough red and white oak cut for at least 2 and maybe 3 more charges (about 300 bf per charge?). I've recently cut some cherry and locust that I'll air dry a few months, so probably have all I can use for this summer. Guess I'll leave a charge in through the winter as well. It might not dry a lot, but it will be out of the elements...?

Good news is I'll have more than I have time to use this winter when I do most of my woodworking - shop is heated, but not cooled. I also plan to move the fan solar panels more to the center for the next charge, as this should give them a bit longer run time as they are partially shaded by the sides.



From contributor J:
Nice job on the kiln. I'd love to know your source for the solar fans. Let us know how the oak turns out when it's finished drying.


From the original questioner:
The fans I used are from Home Depot. They are attic gable fans. I think they were about a 12" fan.


From contributor Y:
Nice job. It appears from the image that that the photovoltaics (PVs) are mounted inside the kiln. If that is true, then you will experience significantly decreased output. They like to be cool. You will get a much better output if you can mount them outside. Another source of DC fans is radiator fans from salvage yards.


From the original questioner:
Thanks for the information. I was going to move the panels anyway, so went ahead this morning and moved them outside the kiln. Cloudy here today, so may not see much difference, but thanks again for the feedback.


From Professor Gene Wengert, forum technical advisor:
Looks great. If you use some of the incoming solar energy to make electricity, then it will not be available for heat, and your kiln will be slower and less effective. So having the electric panels outside and separate from the roof collector is desirable.


From the original questioner:
Wanted to pass along an update. About two weeks ago, did some measurements and had an average of 8.9% MC for 10 readings. Yesterday, checked again and at 7.5% for 10 readings so all in all, looks like it's working well. Will probably pull this load out next weekend if the MC doesn't appear to be getting any lower. Have another load ready to go, so no downtime for a while!

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Kiln Construction

  • KnowledgeBase: Primary Processing: Kiln Operation




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article