Q. We are a jobshop and have a project request for a plaque-sized piece of MDF covered with white primer vinyl with a glossy decal stuck to it. The goal is a high build wet-look gloss finish.

We have tried several different finishes, achieving the best results with an acrylic polyester 50% solids in two coats. This requires 24 hours at 90 degrees for each coat. A faster turn time is desired.

We have looked at UV coatings but can not find one that is clear enough. Waterborns don't adhere to the glossy decal. Laquers appear clear in the can but discolor the white surface when applied. Is coil coating of any interest to us?

A. Bob Niemeyer responds: I suggest you use an acrylic urethane system. This will give you a true water white finish with no color shift. Also gloss urethanes give a 90+ sheen right off the gun.

You may need to use a Barrier sealer (isolating agent) before applying your topcoats due to the different substrates involved. Always pre-test your system first! If you don't have a source for these products try calling ICA Wood coatings at 616-682-9115. Ask for Tim Klinfelter and explain your problem to him in further detail. If you run into a dead end contact me at or at 414-246-6555.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Finishing: General Wood Finishing

  • KnowledgeBase: Finishing: Refinishing

  • KnowledgeBase: Knowledge Base

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2017 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article