Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Attaching End Panels       Methods used by the pros. January 28, 2004

Question
What are you using to attach your finished end panels? Depending on the job (budget), I either screw a 3/4 false door from the inside or use spray contact adhesive and a couple of pin nails to glue a 1/4 skin on. Is there a better way?

Forum Responses
I pin nail 21/4 x 1/4 strips of hardwood to the perimeter of my existing finished ends to give them a Shaker look. It's quick and easy and gives the job a more custom look.



From the original questioner:
What happens if you have a raised panel door? A shaker door wouldn't match.


I usually use plywood the same species as the doors and face frame and lock mitre it. Sometimes I add a door with the same reveal as the cabinet faces. Other times I've made the end panel just like the doors and lock mitred them to the face frames.


Here is my "better" way: buy sheet material with melamine on one side, oak or maple veneer on the other. Cost me just a bit over $40 a sheet. I used to buy a sheet of melamine for $20, a sheet of veneer for $40, and spend half a day veneering the ends. This way I make a better product, save labor and material cost.


Just buy a sheet of 3/4" hardwood plywood and butt joint the face frame to the end panel. Sand and move on. Nobody cares if it's lock mitered or not - the days of plywood face frames that had to be lock mitered to hide the plywood core have been over for 30 years. Mitered ends do look better if you have a paneled or raised panel end.


Using pocket screws from the top and bottoms of the cabinet box into the end panel works well for us. Kreg makes a portable pocket drilling jig that has served us well for awhile now. To cover the holes it makes in the bottom of the cabinet box upper, we laminate a skin onto the underside of the uppers to give a clean and continuous look to the finished product, covering not only the pocket holes, but also the end joints of the cabinets sides as well, if you build your boxes that way.


The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor B:
I am an installer. I have many jobs that have end panels in the form of 1/4" or doors. For me, Liquid Nails and 23 ga. pinners is fast and holds very well. I use a pin nailer made by Grex that shoots up to 1 3/8. Proper placement and angle in the door will leave you
absent of any visible holes on the door or inside the cabinet.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: Commercial Cabinetry

  • KnowledgeBase: Cabinetmaking: Custom Cabinet Construction

  • KnowledgeBase: Cabinetmaking: Cabinet Design

  • KnowledgeBase: Cabinetmaking: General

  • KnowledgeBase: Cabinetmaking: Installation

  • KnowledgeBase: Cabinetmaking: Residential Cabinetry

  • KnowledgeBase: Cabinetmaking: Store Fixtures




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.