Today's
Sponsors:


Mereen-Johnson Machine Company

Merritt Woodwork

MFG in Honduras

Micro Fence

Microvellum

Middle Valley Lumber

Mikron Woodworking Machinery

Mill Outlet

Minimax

Mirror Reflections

MLS Machinery USA, Inc.

MLS Machinery

Modern Woodworking Magazine

Moldingknives.com

Monarch Machinery

Morbidelli

Moulder Services

Moulder Techniques

Mountainside Wood Products

Multicam, Inc.

NAP Gladu

Nebraska Tool

NEMI

New England Kiln Drying Association

NexGen

Hoffmann Machine Company

Holz Her U.S. Inc.

Howard S. Twichell Co.

Hvalsoe Sawmill Ltd.

ICA North America

Icy Straits Lumber

IDM

Impact Search and Placement

Indiana Hardwoods

Industrial Air Solutions

Integra Precision Grinding and Manufacturing

InTrading

Invicta Woodworking Machines

IpeDepot.com

irsauctions.com

Italpresse

J & G Machinery

J and J Barn Wood

J&P Machines

J. Gibson McIlvain Company

Jiffytops

JIT Hardware Supplies, Inc.

JMHsoftware.com

John G. Weber Co.

Joos USA Inc.

KCD Software

Kerber Farms and Mill

Keystone Wood Specialties

Keytrix Data Systems

Kiln-direct.com

Kleiberit Adhesives USA, Inc.

Kreg Tool Company

Kremlin

Lacy Cypress Inc.

Langelier Lumber Ltd.

Leadermac USA

Lewis Lumber Products

Lignomat

Logosol

Lumber Resources

Lumber Smith

M.L. Campbell

MACHINEKING.com

Macoser, Inc.

Mahros

Maine Timber Works

Maine Woods Company

Mann and Parker Lumber Co.

Martin Lumber

MARTIN Woodworking Machines Corp.

Mastercam - CNC Software

Matthews Mill

Maya Positioning Equipment




Buffing out a lacquer finish       Finishers share their secrets for achieving a hand-rubbed lacquer finish. September 6, 2000

Q.
Can anyone help me with the proper procedure for buffing out a nitrocellulose lacquer finish? I'm interested in using rottenstone, pumice and oil.

What is the proper sequence and technique?



Wet-sand with progressively finer grits of sandpaper. It's up to you how fine you want go. You could stop at 400 grit or go up to 600 grit, 800 grit, 1000 grit, 1200 grit 1500 grit, 2000 grit, or 2500 grit. Let's say you want to wet-sand up to 2000 grit. Start your sequence with either 400 or 600 or 800, depending on how much orange peel or pebbliness you need to sand smooth. Then go to 1000 grit or 1200 grit, then 1500 grit, and then 2000 grit.

Use a sanding block, not the flat of your hand.

Then mix up a slurry of pumice. Then you can finish off with rottenstone. Rottenstone is finer than pumice.

When you wet-sand, use a squeegee to check your progress, and check that progress often.

You can use a sanding lubricant made from Murphy's Oil Soap diluted with 75 percent water or more. Or you can use mineral spirits, mineral oil, naptha, or combinations of any or all of those three petroleum distillates.



Are you looking to polish to high gloss or to achieve a rubbed look? If you are doing a rubbed look, short-nap wool carpet works great for rubbing. I don't like using oils to rub with, they just make a mess. I use flax soap, woolwax, or vegetable oil soap as a lube, mixed with water.
Bob Niemeyer, forum moderator


When you say "short-nap wool carpet," do you mean the stuff that we walk on? Could you give me some details how I would use this? I cannot imagine it (I lack the creativity for that kind of mental exercise).

Do you load the carpet up with lubricant or polishing compound? Do you back it against a flat block? And so on...



Bob, I'm actually just trying something new; maybe I shouldn't try to fix something that isn't broken. My finish is good, no orange peel or pebbliness or anything like that, I just want to make my finish look more uniform.

I used a semi-gloss, but I want maybe just a little more sheen. I was curious about using pumice, rottenstone and paraffin oil, and got a response, but am still unclear as to how to apply the "slurry." Do I use the fine grit sandpaper or a rag?



When using pumice (and then rottenstone), a slurry is made by mixing the liquid vehicle with pumice (or rottenstone). Take a small container (those Rubbermaid food storage containers work nicely), and add some lubricant. The lubricant can be an oil-based petroleum distillate or a water-based lube. You can even use straight water with no soap. Then dump in a quantity of powder (pumice or rottenstone). There is your slurry. Mix it to the consistency of pancake mix, maybe a little thinner.

You can rub this abrasive slurry with a rag. But even better than that is to use a large, flat piece of hard felt. Dip the felt in the slurry (or pour some on your surface) and rub in very straight lines. That means you should not arc your rubbing stroke like a rainbow or windshield wiper.

Another method of application is a rubbing brush. I have only heard about this, as this is an old-school method and I had to learn everything on my own. Anyway, the brush resembles a shoeshine brush. I think that these are available online at Ron Ashbey's Liberon.com website. He can also give you tech support on using this method of applying pumice and rottenstone.

It is my understanding that factories are still using pumice and rottenstone in their cutting sequences to achieve certain sheens (to be more precise it is the "look" of certain sheens that they are using them to achieve). But I think that they are using these abrasive materials with pneumatic dual-pad rubbing machines like the ones made by National Detroit and Stuhr (Cooper Power Tools).

It is hard to replicate by hand what these pneumatic machines can do to a finish. Difficult, but not impossible.

I hope that explains a little more. Now let's wait and learn about the artful use of carpeting in the rubbing out of a finish.



For years our shop rubbed all dining table tops. Yes, they looked wonderful, but a couple months later we would get the call to come out and re-rub the top due to mars in the finish. It's like those nice black pianos that are rubbed out; just dust them across the rub and they look awful.

About 25 years ago we started spraying all the final sheens, and the tops held up much better -- no re-calls. What also helped is that we added a slip additive to the last coat so things would slide and not scratch the finish as easily. Now the only time we rub anything out is if it was that way when it came in.

As for the carpet, yes, it is the stuff we walk on. Just get some good, short-nap commercial-grade wool carpet. Cut it to about 4 by 10 inches, then trim back the backer, because even a thread from it will ruin a rub-out if it works its way underneath.

Soak the carpet to get it wet in some soapy (woollube) water, sprinkle a little pumice/etc. on it and rub away in nice, long, straight strokes. You can also place this on a Sundstrand inline sander to do a nice fast rub.
Bob



Go to www.mimf.com and check out what the guitar makers are doing with rub-outs. Guitar finishes are the ultimate in gloss clear and colored finishes. Makes pianos look like non-skid boat decks.


I'm one of those guitar makers (actually I make mandolins), and before I built my very cool buffing system, I got great results using an off-the-shelf auto polish product called Scratch-Out. From the look of it, I'd guess it's rottenstone in a suspension; so fine that it made no difference whether I moved the pad in straight lines or circles. 'Course, I'm working on very small areas (not like a table or piano), and don't know your project.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Finishing: General Wood Finishing

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article