Burlwood Rocking Chair Examples

      Check out two beautiful rockers and the "before" picture of the sawn burls they were made from. May 31, 2010

I would like to cut this ash burl into a couple Luthier blanks. I have never done this. I do have access to a bandmill. Should we cut parallel to the trunk sticking out of the ends, or perpendicular to the log ends? I was thinking cutting two inch slabs that were parallel to the log that the burl is surrounding. The burl is 22" in diameter, and is 24" long. The bark on it is swirly in nature. This is from a green ash tree.

Click here for higher quality, full size image

Forum Responses
(Sawing and Drying Forum)
From contributor K:
The checking is a huge risk. I do not know a way to around it - vacuum dehydration? Wax and seal that baby up and learn as much as you can. I milled some ash slabs. They warped twisted and cracked - ouch! I was just experimenting/learning. Most of it is junk. I would leave it thick so you can cut away the warp/twist. Dry very slow (sealed) and cross your fingers.

From contributor O:
I dried a big burl in one of my vac kilns a couple years ago. It was pretty slow. It took almost a month. It was cut parallel to the trunk and not perpendicular.

Click here for higher quality, full size image

From contributor O:
The burl in my previous post was amboyna. This is what it looked like when finished.

Click here for higher quality, full size image

From contributor C:
Very impressive wow.

From contributor D:
Here is another picture.

Click here for higher quality, full size image

From contributor T:
Burls can be a bear, and they are also a gamble. Cut parallel to the trunk is good advice. End sealing is necessary. Perhaps some overall coating is called for. You never know what's inside until you start sawing - that's the gamble. I have found plenty of rot and bark inclusions, but sometimes you get lucky.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Furniture

  • KnowledgeBase: Furniture: Custom Furniture

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Kiln Operation

  • KnowledgeBase: Primary Processing: Sawmilling

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article