Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Cabinet Doors Tips and Tricks       A start-up cabinet door manufacturer gets some advice on production methods. October 2, 2007

Question
I have just established a cabinet door production facility and have completed my first order of 50 doors. The tools that I used were table saw, Triton router, Dewalt planer, orbital sander, jet parallel clamps, and a lot of hand sanding. I was wondering if I made my stiles and rails wider than desired width. Is there a machine or tool apart from the table saw that can be used to trim to final size? Would a radial arm saw be appropriate?

Forum Responses
(Cabinetmaking Forum)
From contributor J:
Large door manufacturers use double-end tenoners to size doors. For smaller operations, consider over-sizing your doors by 1/8". For example, if your rail/stile stock is 2 1/2" finished, begin with 2 5/8" stock. That way, as the stock moves from rough stock to finished, you end up with 2 1/2" or whatever your finished sizes are. One suggestion, though. If you are going to make a lot of doors, get away from the parallel clamps and get an automatic door clamp. Much faster and you can assemble and pin a door in less than 2 minutes. Also, squaring the door is simplified. Just because you put bessys or jets on a door, doesn't make it square.



From contributor J:
Oh, almost forgot. Voorwood makes a machine that will raise panels and edge doors. The door profiler removes 1/16" per pass, so you would need to oversize your doors by 1/8". That way, when you put your edge profile on, the doors come out the proper size. But this opens a whole other can of worms. For instance, now you are using one machine to accomplish two tasks, which means that as you grow, you will have a bottleneck there. If possible, structure your shop so that you have dedicated machines that perform one task well. It will help eliminate bottlenecks.


From the original questioner:
Thanks for your recommendations and methods for sizing doors. I am looking at replacing the jet clamps with the JLT door clamp, but this will be done when I can afford it. I am experiencing a few doors not being totally squared, but I find when I don't apply too much clamp pressure on the clamps that run in line with the stile, the result is a perfect squared door.


From contributor J:
Are you pinning your doors? That would free up your clamps. What I mean is that after you glue and clamp your doors, shoot a couple of pins (I use a 23 gauge pinner) into the joints. Doesn't hurt to shoot a pin at the top and bottom center of the panel groove to hold the panel steady, too. That way, you can remove the door from the clamp and take it to the next processing station. In our operation, as soon as the doors come off the JLT clamp, we send them through the widebelt to flatten them. Again, good luck!


From the original questioner:
I really appreciate you taking the time to offer your expertise and guidance on building cabinet doors. Incidentally, I am in the process of securing the SENCO kit PC0947 which was recommended by SENCO. This pinner uses 18 gauge pins, and minimum length of pin that it uses is 5/8". Is this okay? I noticed you mentioned you use 23 gauge. At the moment I hold the doors in the clamps for an hour using Titebond Original. Finished thickness is 3/4".


From contributor R:
I rip my stiles and rails 2 3/8'' then add 1/4'' to the length of my stiles, then take off 1/8th on all 4 sides. Table saw for ripping down to width, then a radial arm saw that crosscuts 25'' to cut to height. My doors are square, so this trimming to size is a time consuming precaution that probably is not worth the time, but it's better to be safe than sorry. Space balls are another time thief when it comes to assembly. 3/8'' long brads are needed. Brad them to hold in place. Makes it much faster, then let the clamp override the brads. I don't think brads hold the joint tight enough, but many shops just clamp them, then brad nail, and then unclamp.


From contributor J:
5/8" will work for the joints, but will probably go through the profile if you pin the panels. Also, 18 gauge brads leave a hole big enough to need putty. I use the 23 gauge with 1/2" pins. No need to putty and the 1/2" size works for the joints and the panel. Contributor R's methods work well too. Just remember the purpose of the pins is to hold the joints steady while the glue sets up. There are many different ways to get to the same place. That is why cabinetmaking is so much fun.


From the original questioner:
Okay, contributor R, I'll try your method, but I don't have the radial arm saw, so will probably have to make a sled for the table saw, and hope I can get a perfect 90 degree cut. Where I am located, space balls are not an issue, as movement of the wood is somewhat limited in the tropics as compared to North America. I'll stick with the 18 gauge pinner and see how that goes, as I will only be pinning the joints so that I can remove from the clamps to keep production up. Thanks again for your input, and happy woodworking.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: Cabinet Door Construction




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article