Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Cargo Container Dehumidifier Kiln       Where to put the dehumidifier in a cargo-container drying kiln? January 29, 2009

Question
I am getting ready to start putting together a kiln using an old 40' insulated cargo container and a Nyle L200. What is the optimum location for mounting the unit and fans seeing as the container is narrow and obviously quite a bit longer. I have also toyed with the idea of being able to close off half of the container for smaller loads. The primary use of this kiln is to re-dry or finish drying lumber to a usable moisture content for our own use, mostly softwoods.

Forum Responses
(Sawing and Drying Forum)
From contributor R:
I have a Nyle set up in a container. My dh unit is centered and flush against the sidewall. There isn't much room around the stack when it's loaded. There is just barely enough room to walk by the dh unit - maybe 10-12". My carts are 48" wide. You'll have a hard time setting it up to use only half of the container for small loads. When I dry small loads, I center the stack with the dh unit, and use OSB to baffle the ends of the stack. It works fine.

** NEEDS IMAGWE WORK **

http://www.woodweb.com/images_forums_public/sawdry/kiln_load12.JPG

** NEEDS IMAGWE WORK **



From the original questioner:
If I can ask you another question, how many fans and where do you have them located? My container actually butts up to my building so we will be loading from inside. I am going to mount the controls in the building to prevent from freezing so I need to extend the electrical leads. I considered allowing enough slack for me to pull the unit along the wall for small loads and block off the other half. What do you think?


From contributor R:
I've got five fans that are evenly spaced. I like your idea of leaving extra wire to slide the dh unit. It's not very heavy. I think that would work well.


From contributor C:
I have four fans in my 40' kiln and my unit is on one side. If I were to do it again I would mount the unit in the center and on the outside and duct the unit to the container. It is much easier to service and no chance of hitting the unit during pulling the lumber carts in and out.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Kiln Construction




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article