I have to build 30 tabletops out of 5/4 beech, which I never worked with. I'm wondering the general properties of this wood, mostly how stable it is as far as cupping? The lumber looks great as its straight and flat. Also, should I use a WB finish (Agualente MLC) in a restaurant application?

Forum Responses
(Furniture Making Forum)
From contributor P:
The Euro steamed beech has been wonderful for me. I've been using it for cabinets, furniture, and on the grill. (It makes a dandy smoke when soaked in water for a day or two).

I'd not be hesitant to make tabletops with it. I've made a ton of doors using it for the frames and panels and I think it's one of the easiest woods to make doors with at the price. It's pretty hard, glues well, and takes an edge well. It looks great distressed and the color is very consistent. It takes a little more effort to sand because of the hardness, but doesn't fuzz around knots or swirls like a softer wood.

I have only used a few boards wider than 6", but I had no cupping or warping problems. Of course you still need to take care to not use any pieces that are likely to cause problems, but in my experience, I've had a lot less waste with the beech than with other woods like alder and oak.

From contributor J:
I used it for numerous kitchen cabinet jobs, built-ins, glue ups for large drawer fronts etc. I really like working with it. It's a dense wood so glue penetration is basically the same as working with white maple. My only suggestion is to not over tighten the clamps on a glue up. I had several face frames pop loose on the finished ends (as I don't face nail and clamp only on finished ends on cabinets) on one cabinet job. This happened during the winter so cold was a factor. I have never had the problem repeat itself. I tend to over tighten my clamps, so for beech I use more clamps and less pressure.

From contributor D:
Great wood to work with and for the price it is awesome. I dont expect prices to stay down once everyone discovers it. Contributir P - can you use it for smoking? I thought they chemical steam it to stabilize it? Is it a good outside wood?

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Furniture

  • KnowledgeBase: Wood Engineering

  • KnowledgeBase: Wood Engineering: Wood Properties

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.