From contributor H:
If you want to use this type of clamp - we do, and they work well in numbers - make your own. Buy a ten foot length of 3" or 4" CPVC DWV pipe. Cut to desired width on saw. Wide = stronger clamping. Route small bevel edges using table mounted router. Split ring on band saw. You can make them for a fraction of the price in the size you need.

From contributor A:
I lose count of the number of miles of bevel edge I have put on in my time. But in my opinion, packing tape is still the fastest. The above clamps are great, I am sure, but seem cumbersome to set up.

From contributor H:
We don't use them for bevel edge either. We use them for SS edges.

From contributor G:
Tried using edge clamps and what not before. Just too big of a pain to use, and to buy them as advertised... whoooeee! I'll stick with using tape.

From contributor K:
Be careful! I made fun of Dani Clamps for years believing, as most people wrongly do, that they are made from a Std PVC pipe. At one point I was forced to use some from someone else to do an emergency repair (a whole other story). I was stunned by their performance! Then I began to research the whole matter. I tested PVC pipe vs. Dani Clamp. Immediately the differences were obvious. The PVC was inconsistent in performance (foot #'s), with poor memory. I found Dani to be the exact opposite. Next, a check to OSHA. If you are not set up to work with PVC in your shop and have an injury or FED visit, you're screwed. There are a lot of guidelines to working with PVC, which have just been recently tightened again, that are both health and safety driven. My shop insurance does not need to be raised. Check the differences before you speak. I know I'm still eating Crow.

From contributor M:
How do you apply the tape? Wrap around the countertop? It seems it would want to push the edge up. If you don't get a perfect glue-up, any trick to smoothing the edge? I just received my first Kuehn bevel edge and will be assembling it day after tomorrow, so any tips are appreciated.

From contributor A:
The way I like to do it is to put a strip of tape running along the edge of the top. This way, when it is time to remove all of the little strips of tape, I just pull this one long one and it takes the rest with it. Use good quality tape. That cheap crap tears and this method, then, is actually more work. The other option is to leave a little tail to grab onto on each individual piece.

As far as the edge riding up, for about every 5 or so pieces, I will put one piece running under the countertop. This helps to keep the edging down as well as ensuring a good bond along the bottom edge.

To smooth, take a short drop off and rub the corners with it pretty hard. Some of the print from the scrap will rub into the gap along the top filling it in and evening it out. This, of course, doesn't work for glossy laminates or the new Wilsonart HD series. Actually, I guess it isn't all that new anymore.

From contributor U:
I use the flat back edge and tape it every few inches with strapping tape (the one with strings in it). When you apply it, try to pull the tape straight toward the countertop. If you tape the bottom and then pull it up, the edge tends to want to creep up from the tension. After taping, wipe all the glue squeeze out off with a wet rag (the glue under the tape will not dry fast and can be wiped off after you remove the tape). Next I rub some Seamfil along the edge and in the joints, and without cleaning it off, I smooth the edge. To smooth the edge I use a piece of bevel edge scrap or the round shank of a screwdriver to burnish it. My thinking is this sort of rolls the edge over and traps the Seamfil in the joint. It also smoothes it out. Then I clean it with lacquer thinner and do any final touch-ups. I sometimes use some real fine sandpaper about 400 grit to smooth any sharp edges that are left. Do not use your laminate file to smooth the edges, it is too aggressive and you will file through the laminate color very quickly.

From contributor V:
Set your router correctly and the packing tape works fine. We have done miles of the stuff this way. Don't forget to get a few packages of Band-Aids because that stuff is sharp.

The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor S:
If your build-up is no wider than 2 1/4 to 2 1/2 wide, you can use the 3" wide opening spring clamps. This holds the bevel edge (with tongue) down and against the front while drying, plus you won’t have any tape across your glue line. I use a 12" piece of 3/8" chrome supply line and run it across a fine wire wheel to rough it up. This heats the plastic as you burnish it across the top edge.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Laminates and Solid Surfacing

  • KnowledgeBase: Laminates & Solid Surfacing: Fabrication Techniques

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article