Today's
Sponsors:


Mereen-Johnson Machine Company

Merritt Woodwork

MFG in Honduras

Micro Fence

Microvellum

Middle Valley Lumber

Mikron Woodworking Machinery

Mill Outlet

Minimax

Mirror Reflections

MLS Machinery USA, Inc.

MLS Machinery

Modern Woodworking Magazine

Moldingknives.com

Monarch Machinery

Morbidelli

Moulder Services

Moulder Techniques

Mountainside Wood Products

Multicam, Inc.

NAP Gladu

Nebraska Tool

NEMI

New England Kiln Drying Association

NexGen

Hoffmann Machine Company

Holz Her U.S. Inc.

Howard S. Twichell Co.

Hvalsoe Sawmill Ltd.

ICA North America

Icy Straits Lumber

IDM

Impact Search and Placement

Indiana Hardwoods

Industrial Air Solutions

Integra Precision Grinding and Manufacturing

InTrading

Invicta Woodworking Machines

IpeDepot.com

irsauctions.com

Italpresse

J & G Machinery

J and J Barn Wood

J&P Machines

J. Gibson McIlvain Company

Jiffytops

JIT Hardware Supplies, Inc.

JMHsoftware.com

John G. Weber Co.

Joos USA Inc.

KCD Software

Kerber Farms and Mill

Keystone Wood Specialties

Keytrix Data Systems

Kiln-direct.com

Kleiberit Adhesives USA, Inc.

Kreg Tool Company

Kremlin

Lacy Cypress Inc.

Langelier Lumber Ltd.

Leadermac USA

Lewis Lumber Products

Lignomat

Logosol

Lumber Resources

Lumber Smith

M.L. Campbell

MACHINEKING.com

Macoser, Inc.

Mahros

Maine Timber Works

Maine Woods Company

Mann and Parker Lumber Co.

Martin Lumber

MARTIN Woodworking Machines Corp.

Mastercam - CNC Software

Matthews Mill

Maya Positioning Equipment




Color and Shade Issues in Book-Matched Veneer       Sawing can create a "light side" and a "dark side" on veneer pieces, leading to visual appearance issues in bookmatched veneer layups. Here are some explanations of the issue and some suggested solutions. July 26, 2005

Question
I have been book matching veneer, and I am wondering how to deal with color issues when book matching center-match positive and negative veneer. One stave looks different from the other in color and I’m not sure why. Does anyone have any suggestions?

Forum Responses
(Veneer Forum)
From contributor J:
The light/dark is caused by one side of the veneer being open or broken. This happens during veneer cutting and is referred to as tight side/loose side. Place veneer between the palm of your hands and twist your hands, you can feel the difference.

Two things you could do are:

1. You can treat the veneer with glue siz. This helps to balance the absorption of top coats and finishes, leading to a more uniform appearance (Notice I did not say balanced, perfect finish).

2. You can eliminate the light dark issue of book matching by using veneer that has been cut on a lumber slicer. This method of veneer production does not result in loose side and tight sides.
Both surfaces of the veneer are the same.



From contributor F:
Contributor J is right on the money. You can also consider slip matching instead of book matching, and that will avoid the tight side/loose side and barber pole effect that is common with a book match.


From the original questioner:
What is slip matching? The architect requires book match. Is it similar? Or is it similar to sequence match?


From contributor J:
Slip matching is joining the leaves in sequence without flipping every other one.


From contributor L:
To contributor J: I searched the site and found several other mentions of lumber slicing, but no explanation as to what it is or how it's done. Is it slicing off pieces thick enough to class as lumber? Is such veneer common to find or a specialty item?


From contributor F:
To the original questioner: I would guess that the architect doesn't know the difference, he's heard book match and that's all he knows. If looks and sounds like a solution someone will have to enlighten the architect. Slip matching is less common than book matching, but slip matched sheets and faces are usually available from stock in many species from most veneer converters.


From contributor F:
I should have gone a little further. What is the species, and what is the cut that the architect has specified? This may have a bearing on a decision or direction. In fact, has the cut even been mentioned?


From contributor J:
To contributor L: You can see a lumber slicing video by doing the following

Go to:
www.fezer.com.br/eng
Click - products
Click - digital video
Click - slicing wood
Click - FM30

Here is what you are looking at. Imagine six pieces of wood going around in a circle - as veneer is peeled off, it is placed on the corresponding pile to keep it in sequence. The boards are taken across a knife which is at 75 degrees to the wood, and the veneer is peeled off of the bottom.

The pressure system is like a tank track made of rubber (like a giant rubber belt), and it transports and holds down the board across the knife. This system of slicing produces higher quality veneer than traditional methods.



From contributor K:
I believe the barber pole visual effect of book matching is due to reversed grain direction rather than the method used to produce the veneer. I have observed the same thing on book matched re-sawn veneer. The degree of contrast varies with the angle of the wood fibers to the panel surface. Slip matching will produce a more consistent look. Glue size or a wash coat of finish before staining may help to reduce the contrast.


From contributor C:
I agree with Contributor K. He described well what causes barber-poling. It is a side-effect of one of the properties that makes wood appealing: chatoyance, which is just a good Scrabble word meaning "changing luster" - sort of a mild version of one of those hokey 3-D pictures with the layers of polarized plastic on it. It is not a function of veneer manufacture, but the effect of light refracting differently off of the two (or more) leaves of veneer because they are flipped in opposite directions.

Some species, cuts, and figure types are more likely than others to result in barber-poling, but it also varies log by log and flitch by flitch (Contributor K's explanation should make it clear why).

As a side note, I've seen barber-poling used intentionally for aesthetic effect. I don't usually associate walnut with barber-poling, so changing flitches might be one way to deal with the problem. As the others have said, other solutions include changing the match and changing the architect/designer's mind (good luck).

As far as glue-sizing and wash coating in the finishing process, I doubt it will be successful if the barber-poling is extreme. The goal would be to kill the wood's chatoyance, which can be done, but I suspect that these two methods won't go far enough.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Veneer

  • KnowledgeBase: Veneer: Processing And Manufacturing

  • KnowledgeBase: Veneer: Techniques




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article