Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Comparing moisture meters       An assessment of the performance of pin and pinless moisture meters made by major manufacturers. July 11, 2000

Question
I need some help selecting a moisture meter. I just got a new bandmill and plan on milling a lot of lumber. I also plan on air-drying quite a bit of wood.

My main use of the meter will be in measuring rough lumber, but I am still concerned about the pinholes showing though, after planing the wood. I am debating between the Wagner L606 (pinless) and the Delmhorst J-2000 (pinned). They are the same price.

Are these good meters? Any others I should consider? Is there one that is both pinless and pinned?

Forum Responses
Electrophysics. They have a dual mode (pinned and pinless) meter for $330. Anyone have experience with it?



Do I understand that you will be using these meters on air-dried lumber? Why? What will you do with the info?

I think that you will have very expensive meters but the need for accurate data is limited. When you go into the kiln, you will have to cut normal moisture content (MC) sections. If you use a solar kiln, then the entering MC doesn't matter. In short, I do not think that you need a meter for air-dried lumber.
Gene Wengert, forum moderator



From the original questioner:
After the lumber is air-dryed, I want to bring it into the shop (which is the same temperature and humidity as the house) and let it finish drying.

I want to use the meter to see how far along in air drying it is, and then how dry it is once it has been in the shop for a while.



Gene's reply:
In that case, it seems that knowing the MC gradient would be especially critical for you, so the pin meter would be a good idea.

Actually, if you can afford both, you will find them both to be useful -- I like to suggest that about $200 is the minimum price to pay for a good meter. I also suggest that you get one that lots of other people use, to help in learning how to use it, special techniques, etc.
Gene



I have one of the Wagner pinless meters, and I'm using it to monitor MC in the yard, the solar kiln, the storage barn, and the furniture workshop. It's easy to use, has been accurate the few times I've had a way to check its calibration and the adjustment tables, and leaves me feeling confident in the MC of anything I'm about to use.


Regarding Electrophysics' moisture meter: I have both a pin and pinless. They are very reasonable in cost (under $200). My company also has two Delmhorst meters.

I have had very good results with the Electrophysics meters. They are fast, easy and reasonably accurate. In some cases, I have found them more accurate than the Delmhorst, when compared to oven samples.
I would be interested in hearing other comments. Currently, I only use the Electrophysics for quick checks, but would consider using them for more if they were industry accepted.



I did compare over 150 kiln-dry samples with the pin (Lignomat and Delmhorst) and the pinless (Wagner) meters. Although any one reading could be off, on the average all three meters were very close.

For example, the error was .5 percent, .7 percent, and -0.1 percent MC for the three meters on hard maple; .6, .5, and 1.2 on red oak; and .3, .9, and -0.1 on walnut.

See the Forest Products Journal Vol. 47, No. 6, pp. 60 - 62 for details. (These results are very good considering that the pin meter measures in a specific spot, the pinless in one half of the thickness, and the oven test in a large piece.)
Gene



The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor J:
Many people seem to think that meters with pins are more accurate. They would be suprised to learn that pinless electromagnetic wave technology is more acurate and does not damage the wood. It is also easier to use in professional and private atmospheres.



Comment from contributor M:
The pinless or inductive moisture meters are more subject to interference (from things like metal) and are not reliable when used in any construction that involves nails, screws, pins, metal fasteners, etc. So, except for measuring moisture at the lumberyard, they are not a first choice. Also, I've seen widely divergent readings from inductive MM in the same location when taken one after the other. I'm not really a fan of Pinless either.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Primary Processing: Air Drying Lumber

  • KnowledgeBase: Primary Processing: Kiln Operation

  • KnowledgeBase: Wood Engineering: Wood Properties

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article