Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




Confirmat screw assembly       Troubleshooting problems with Confirmat screws. June 24, 2002

Question
I'm easing into frameless cabinetry, using Confirmat screws as the assembly method, but I’m not sure that these are the way to go. I’m low on funds, so I don’t have a lot of choices.

I've gotten a few sample screws and purchased a "step" drill bit. I am not impressed with the specifics of the bit. First, it's about 4-1/4" from tip to the end of the flutes. Because the screws are only 2 inches (50mm) in length, it would seem that I only need a bit that is slightly over 2" in cutting length. The drill is very coarsely milled and it is actually tapered, rather than stepped. I don't see how I can very easily control the proper depth of the hole to accommodate the length of the 5/7/10 - 50mm screw. I don't believe a drill bit stop will work on this bit.

Anyway, I gave it a try on some 3/4 VC ply scraps and found the bit to require a tremendous amount of effort to feed. When it reached about an inch and a half into the material, the plywood core split wide open - even before I reached the 7mm step (or taper). I recognize I was probably too close to the end with this sample test, which encouraged the blow out. I plan to build using mostly 3/4 VC ply but will also move into some work with pre-finished PB panels, and possibly even some MDF core products.

My Hafele rep tells me this is the correct bit for these screws and the Confirmat system. Surely there is a better single purpose bit on the market for drilling holes for the common 5/7/10 x 50 Confirmat screw. I've posted a picture to show what the bit looks like and the results I achieved on my virgin attempt to use these fasteners. I could use some help sorting out the particulars of this fastening system.

Forum Responses
From contributor F:
First, a Confirmat type screw is made for particleboard, not plywood. The bits are also made for the more consistently dense particleboard. Second, consider pre-drilling for the screw body or shank ("stern" GR) in the flat component and the screw portion, minor diameter of the screw thread in the end drilled component. Drilling depth is then only an element of the end drilling and not very critical. Then use an assembly screw with nibs for the countersink and set your torque limit for depth. Confirmat type screws are available with a pointed end or flat end in addition to nibs or no nibs.



From the original questioner:
I suspect that PB core and particularly MDF would split more easily than well-glued up ply. I certainly have driven many screws (made for PB) into the end grain of plywood and, with the proper sized drill, had no problem with splitting. Aside from that issue, if these fasteners are only designed to work with PBC products, I am prepared to restrict them to those panel products.

I have been building VC ply (face frame) cabinets for some 11 years now and have used various methods of assembly - predominantly dado, glue and nail guns for the boxes, pocket holes for the frames and glue and clamp (with a couple of well placed nails, per frame, for added mechanical reinforcement) for fastening frames to cases. There must be a "stepped" bit that will allow drilling for the common sized Confirmat screws in a single drilling operation. I have considered drilling in two and even three steps but that will not do for the intended production efficiency I had hoped for.

I did see that these screws come in various sizes, to include pointed ends. If the nibbed heads of these screws are anything like the other nibbed headed screws I've tried, I'd prefer to counter sink for the head and ease the screw in its predrilled location. I will certainly try them, but one of the features of the Confirmats I was looking forward to was for use in KD furniture – bookcases, etc.



From contributor M:
I have a lot of experience with Confirmat screws, so here it goes.

The drill that you show is a Hafele bit that is supposed to be used in their Zentrix manual drilling jig - that is why it is so long. The jig locates the bit in the center of 16,19 and 22mm sheet goods and stops it at the proper depth. It makes very quick work. The jig works well but is very pricey.

You can use the step bit alone in a drill as shown, but be careful as these bits are very fragile and easy to bend if they jam in the wood. I've made a stop collar (for the bit shown) out of fuel line tubing going from where the chuck stops on the bit to the depth that I wanted. This is so the stop never moves up on the bit. I think that the tubing is 3/8" inside diameter.

I have also seen much shorter step bits, including carbide tipped, but I have never used them. When I find a source I will try.

As for the blow out on plywood, you can expect the veneer layer to chip close to the edge of the panel - this happens to me all the time.

Also, look under custom cabinet construction in WOODWEB's Knowledge Base for more Confirmat info.



From contributor F:
Splitting MDF or particleboard is a non-issue if the right size bits are used. The thread design is made for the application. Confirmats, by any name, were developed particularly for particleboard. The correct hole size allows only the threads to engage the substrate. The step drill bits are very expensive and fragile. The use of separate bits for each member is better for alignment and easier on the pocket that finances your tool purchases. No stop is really needed and nibs only eliminate an operation.


From contributor B:
According to the picture, it appears you are using either fir plywood or some really bad birch. Either way, I don't think you're giving the Confirmats a fair shake. I use Confirmats exclusively to assemble cabinets, and simply don't have problems with board splitting. I employ the method mentioned by contributor F. I bore a 5mm hole in the horizontal piece and a 7mm hole in the vertical piece and use the nib screws to countersink. I don't have any problems. The step drills that Häfele sells are very expensive.

If you are considering making the move to frameless construction, run - don't walk - away from veneer core board. It's too inconsistent. Voids can cause problems in the bander, as well. I use thermally fused melamine on a particleboard core. Again, with the proper sized predrilled holes, splitting is a non-issue. I don't use MDF for case parts simply because it's too heavy. MDF does, however, make an outstanding substrate for doors.

One other comment on your test - AWI does not allow European assembly screws to be closer than 36mm from an edge.



From the original questioner:
Contributor B, I take it that you and contributor F use two separate bits to drill for these assembly screws. Do you have any trick methods of making sure both holes align with each other so that when the screw drives into the horizontal panel, both parts mate perfectly at the edges? Though you haven’t specifically said so, is it as simple as clamping/holding the two parts together and drilling the 5mm hole through both parts, then removing the end panel or V-partition to enlarge that hole to 7mm? If done in two stages as described above, seems like the hole will blow out on the back side when drilling the 7mm hole through the existing 5mm hole, unless a backing is provided to support the exiting drill - more time. And then, if you already have the two parts clamped and mated perfectly, why would it not be best to drill (with at least a two-step bit) to ensure precise alignment at assembly?

If I had two drills set up, one with a 5mm bit and the other with a 7mm bit, I could drill the 5mm hole through both parts to the final depth, then pick up the drill with the 7mm bit and bore out the vertical part to a depth that (at least) clears the thickness of the V-part. I don’t reckon if I bore 1/8” or so into the horizontal part, that it would make much difference. Insert the screw and go on to the next, making assembly as the parts are clamped only once. Am I on the right track?

Drill bits come in various styles, end shapes, milling configurations, and metallic composition. What specific metric bits do you find cut cleanest and last longest?

As a side note, the plywood in the image is a high-grade 7-ply white birch that actually measures a consistent .750 and is virtually free of voids in the core area. Of course that varies some as the relative humidity in the shop changes from week to week, but as all panels (except the top one) change fairly consistently, the job progresses without difficulty. A closer look at these scrap pieces revealed that they came from a batch of plywood from a job I did several months ago. The core is made up of some very hard and heavy exotics, which I believe contributed to the difficulty in drilling and promoted splitting with this particular drill bit.



We have used a 5mm bit for the edge bore and 8mm for the through-bore hole. This gives you a little play during assembly. For a recent run of RTA fixtures, we special-ordered the exact diameter pilot bit recommended by Hafele (5.4mm if I recall correctly), which makes splitting a non-issue in both PB and VC ply.


Confirmat screws were developed in Germany for KD type furniture, either MDF or PB, not plywood.

A hammer is for driving nails. A Confirmat is for the above. A dowel is for frameless cabinetry... done the right way.



From contributor G:
Contributor B can drill two differently sized holes with speed and accuracy because he has a machining center. If a CNC is a bit out of your league right now, try this.

Assemble the boxes with staples first. Now strike lines where you want your screws to go. Remove the edge guide from the zendrix attachment so the face of it will sit flat on the material (the edge guide is very handy if you will always be drilling on the edge of your work, but makes it impossible to drill for drawer stretchers, partitions, etc).

Pull back on the spring-loaded slide of the zendrix guide so the bit is exposed. Put the tip where you want it and let the guide spring back to the surface of the cabinet and drill the hole.

Contributor M has a good idea for a drill stop, but I’m not sure that it will give you guaranteed perpendicularity to the surface, which is essential.

These drills create a lot of dust and much of it can wind up right back in the hole. That’s why the drill is deeper than the screw.

Since the cost of the zendrix system has apparently gone down so much, it might be advisable to get two guns. One would have an edge guide attached and the other as I described above.

One last note. It’s been a number of years since I’ve actually used melamine (and therefore Confirmats), but I never had luck with the carbide drill bits. I found them to be very brittle.



From contributor M:
The zentrix drill guide is great for drilling holes along a cabinet side. It locates the holes the correct distance in from the edge of the panel. When I need to drill the hole in the center of a panel for a partition, I do it freehand with my bit with the tubing stop, no zentrix jig. The straighter the bit goes in, the better, but I have had no problems with a slightly tilted hole as long as the pieces are aligned when the holes are drilled.

If you're going to use the Hafele bit to freehand drill, I've found that you must hold the pieces tightly together or the bit can self feed very quickly and cause the side panel to jam and bend the bit - a very expensive mistake. You can use nails, staples, corner clamps, etc. This is not a problem with the zentrix jig.



From contributor R:
We only build frameless European cabinets based on the 32mm system.

Double-sided thermally fused melamine is a superior product compared to veneer core plywood at half the cost.

There is one option to consider over Confirmats. Try the Hafele Zip-R screws. They require no pre-drilling and hold like crazy. I use the #10x2". I made up several test samples and compared to Confirmat and simple wood screws. The Confirmats held very well but could tell no difference from the Zip-R's and the Zips eliminate the need for expensive, fragile step bits. Of course, I don't build my cabinets for RTA or take down. If I did, the Confirmats would be the way to go. And if I recall, that's why they are used in Europe. When people move, they take down their cabs and take them with them. Not likely to happen here.

And I disagree about dowels being superior in mechanical holding strength to any screw. I recall reading that a comparable screw has 450% more holding surface than a dowel. Although I agree that dowels will eliminate the need for end panels, we use raised end panels about 98% of the time anyway, so that's a non-issue.



From contributor K:
Have you used the Zip-r screws long enough to know there is no board splitting when you don't pre-drill? Every time I've tried the latest "no pre-drilling required" screw, something would split or there were bulges at the edge. I would be tickled to find a no-drill screw that actually does work. (Although, since I use 5/8" melamine board, I suspect I will have to continue with Titus hi/lows and pre-drilling.)


From contributor B:
First, if you are attempting to drill with two separate bits, in two different operations, boring machines are necessary. Don’t try this with a hand drill - you will be terribly unhappy with the results. I’m boring with a Busellato P2P. The same results can be achieved with manual boring machines, preferably with two separate machines. I’ve never been a big fan of the convertibles. Attempting this with a hand drill will be slow and not very accurate.

If you want to use a hand drill, staple and screw is my preferred method. It’s much faster than using the Confirmats. It is not as strong, but you’re building kitchen cabinets - how strong do they need to be? I guarantee that even using staples and screws, the joints will be far superior to dowels. I cannot personally attest to using a #10x2” screw without the material splitting out. I can attest to using a #6x2” in 3/4” two sided thermofused particleboard, with no problems. I did pre-drill a 3.2mm hole in the side to help with part location as well as help get the screw started. I used the Hafele Zip-R’s as well.

In my opinion, 5/8” material is a complete waste of time. 5/8” offers no positives over 3/4”. It’s not going to save much in weight. In some cases, it can actually cost more, particularly when you get away from commodity colors, and there’s also the issue of screwing and doweling.

How are you going to bore for your hardware? Assembling the cabinet is the easy part. Boring for the hardware is the critical part. You can easily slap four pieces of board together to make a box, but if the doors and drawers don’t fit in it, it’s going to be a trying time.



From contributor K:
Contributor B, the 15 lb. difference between 5/8" and 3/4" melamine board (4'x8') is not too much if one is young. Carrying 20 or so sheets of 3/4" board to the saw in the course of cutting out a job would probably result in the need for a colon tuck.

Strength and durability are satisfactory with 5/8 as long as spans are considered. A couple of large dental suites I built in 1985 are still in good shape. (But when necessary, I buy 3/4 and just grit my teeth.)



From contributor R:
Contributor K, I have been using the Hafele Zips for 14 months with no problems. I did error on the size. We are using the #6x2". No pre-drilling and no splitting and no bulges. I wouldn't use anything else. They countersink very well, too.

Also, because I use 4x8x3/4 sheets of melamine, I purchased a panel cart from Hafele. No more back pains. You can rotate it from horizontal to vertical, slide the sheets on, about five or so, and rotate back to horizontal and lock. Then wheel it over to the panel saw and slide the sheets right onto the slider. A breeze!



From the original questioner:
A little more background… First, I have a better than average understanding of the 32mm system and basic construction methods of frameless cabinetry, considering I'm in the face frame cabinet business. I've even built several frameless style bookcases, wall units, and vanities. For these I used a combination of dados, glue, nails and other mechanical fasteners – I don’t think I used any one of these methods twice. I would consider none of these methods for using on a production basis for cabinetry. They worked, but all had drawbacks. All my troubles would be over if only I had the space and money for a construction/line boring machine.

I have always used Euro hinges and Euro slides of several configurations and from several manufacturers. I bore all my doors with a small Mepla hinge-boring machine. I have always drilled wall units for adjustable shelves. I have always applied wood tape to these shelves. Plant-on (usually 5-piece to match the door design) end panels are common on my finished ends. I have constructed dovetailed drawer boxes and doors but prefer to outsource them on all but the smallest of jobs. I have done about every degree of overlay you can imagine, even to the extent of full overlay - so that you would think the cabinets were frameless, until you open a door. Inset doors and drawers (1/6” reveal) are my specialty and here is where I had to really learn what square is. Okay, not “CNC” square, but as square as humanly possible.

I have what it takes to bore accurate system holes (albeit slowly) for doors, drawers, hinges and shelf pins. I have used the Euro leg levelers on a few jobs in the past - the ones that adjust from inside the cabinet and allow the toes to be clipped on and off the legs. I do certainly have a lot to learn about the details of frameless cabinet construction. Without the ability to drill for dowels (I believe it's called "construction boring"), I'm most concerned with the best method for me to join components, given my equipment and available funds.

I don’t have one of the Zindrex guides and so will try the 6x2 Zip-r screws. They are available in square drive, which I prefer. There is another specialty screw that I see in the Hafele catalog - the SPAX Screw. It’s uni-drive (square/pozi pecess), synthetic coated, no predrilling, aggressive grab threads with patented cutting threads. Anybody try them yet?

There are a few commercial jigs and manual systems on the market that make it possible to accurately drill system holes for Euro hardware. I have been through most of them and have settled on a couple that work accurately for me. And as I mentioned earlier, I use the Mepla hinge boring machine for door hinges. Of course, it all starts with parallel edges and square panels – without which, none of this matters.

Could someone point me in the right direction for looking at manual boring machines?



Contributor G, it boggles my mind to think that anybody actually builds cabinets with staples, then marks the box and drill holes with a hand drill, inserts a screw - and makes any money at it. How is that possible?


From contributor G:
Be boggled no longer. Several years ago, I did a time study on how long it took me to assemble a box using the method outlined above.

Using all 3/4” material (including backs), the process takes about 13 minutes per cabinet. In terms of profitability, myself, one full-timer and one part-timer produced over 500K in sales last year.

Note to all: a number of posters have sung the praises of melamine over plywood. Yes, it’s cheaper, it’s easier to clean and it has a greater yield due to not having to deal with grain orientation. Only problem is that it’s not wood.



From contributor F:
Contributor G, you may get an argument on the definition of "wood" but not from me, or at least not today. Are you a cabinet maker or a log hugger? The artisan viewpoint fades when a profit motive becomes the focus.


From contributor B:
Not too long ago, I did a favor for my sister-in-law. Her office wanted a little break area. Simple 8' straight deal with a sink and some wall cabinets. They wanted cherry slab doors. I couldn't readily get my hands on either MDF or PC core cherry for the doors (no matter what you buy here, it's a melamine box), so I got a piece of 3/4" cherry VC core. I cut the doors and attempted to band. The problem was a void all the way across the first layer under the veneer. As it ran through the bander, the pressure wheels indented the veneer into the void. I ended up going through three sheets to get the job done.

I build commercial and institutional exclusively. Probably less than 20% is wood. In this end of the industry, melamine is the standard. I also use a fair amount of cold pressed HPL. At any rate, even if the cabinets have wood doors, they still have some sort of laminate box (unless they are open cabinets, in which case I use veneer laid up on PC core).

Nothing looks better than a natural finished maple interior, when it's new. I've got natural finished maple interiors in my house, natural finished red oak dovetailed drawers, the whole deal. My house is seven years old and I've got a 6 year old and an 8 year old who help me do dishes, cook, etc. I hate the natural finished stuff. Finished materials just don't wear like melamine does. I have laminate in my bathroom and laundry room and I love both units - they've held up well.

Particleboard seems to have a bad rap. The vast majority of the public is uneducated about it. The only thing they know is that cheap entertainment center they bought three years ago was the worst piece of junk they've ever seen. But I'm talking about thermally fused melamine. When was the last time anyone at this forum can recall a piece of melamine delaminating? We've used it for almost 20 years and I don't remember a single piece. I can't say that about plywood. Same thing goes with cold pressed laminate. I have seen some problems, but never with my supplier. It's pretty difficult to screw up spreading PVA on a board and pressing a piece of laminate on it. These things need to be explained to the customer.

Contributor G, have you ever stained veneer that was on MDF or PB core? MDF is hands down the most consistent staining substrate on the market and PB runs a close second.



From contributor G:
Contributor F, no argument insofar as the need to make a profit is concerned. I am fortunate enough to be in a niche market where my clients have very deep pockets (the project I’m just finishing now is currently on the market for a cool 23 million). So even though I use top shelf materials, it is still a pretty small portion of the selling price. Without a doubt, guys in more competitive markets have to find a way to reduce costs and using melamine is one of them.

Contributor B, architectural veneer panels are supposed to be void-free in the two outermost layers of their cores. Sounds to me like you were sold second-rate goods.

No sprayed finish (except perhaps polyester) is going to out-perform melamine in the durability test. Still, it seems like your wood cabinets should have stood up better. Did you use a catalyzed finish like Duravar?

Finally, lest anyone regard me as an “It’s got to be all wood or nothing at all” snob, I use ranger board (MDF) on all of my center panels on my paint grade work. You can’t beat it.



From contributor B:
Contributor G, just to clarify, in my sister-in-law's project, I just needed a couple of pieces and ordered Columbia's board from the local distributor. On a typical job I would order custom laid up panels.

As far as my cabinets at home, the real problems are in the utensil drawer, where it's common for the utensils to be a little wet or me to have wet hands while going for one. Same for the junk drawer and my pot and pan rollouts. My drawer vendor, at that time, used Jellico's pre-cat varnish. The cabinets themselves have held up. We used Guardsman's Super Chem-Veer post-cat - in my opinion the best on the market. The point I was trying to make is the melamine in the Meta-Box drawers does not have the wear and tear.



The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor A:
I have been doing frameless for some years. 5/8 melamine is the standard here. I have tried most of the methods discussed and after several years I use a #6 x 1 3/4 particleboard screw. I pre-drill during assembly. I use finishing gables on all exposed ends. If you're a small shop doing a couple of kitchens at a time, this works very well and is cost effective.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: Commercial Cabinetry

  • KnowledgeBase: Cabinetmaking: Custom Cabinet Construction

  • KnowledgeBase: Cabinetmaking: Cabinet Design

  • KnowledgeBase: Cabinetmaking: General

  • KnowledgeBase: Cabinetmaking: Residential Cabinetry

  • KnowledgeBase: Cabinetmaking: Store Fixtures

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article