Today's
Sponsors:


Vintage Wood Products

VortexTool Co. Inc.

VyTek

W. Moore Profiles, Ltd.

W.L. Fuller

Wagner Electronic Products

WalzCraft Industries

WEIMA America, Inc.

Weinig Group - USA

Western Dovetail

Williams and Hussey

Wisconsin Knife Works

WMIA

WMMA

Wood Doctor's Rx, LLC

Wood Technology Inc

Wood-Mizer

WoodCabinetDoors.Com

WoodenBoat

WoodFinder

WoodJobs.com Search Consultants

WoodLINKS

Woodmaster

WoodPlanet Inc.

WoodSprayGuns.com

WOODWEB

Woodworker's Supply/woodworker.com

Woodworker's Directory

Woodworking in America

Wright Timber

Specialtytools.com

Speed Sander

Spink Lumber

Sprayguncaptain.com

Stefani

Steve H. Wall Lumber Co.

Stiles Machinery

Stiles Shop Solutions

Stoneys Hardwoods

Super Source Tooling Inc.

Supergrit Abrasives

Superior Wood Products

T-Tool USA LLC

Target Coatings

TaylorCraft Cabinet Door Company

Techno CNC Routers

Template Services

The Veneer Store

Thermwood Corporation

Tiger Wood Ltd.

TigerStop

TigerwoodDecking.com

TimberKing

Timesavers Inc.

TMS Machinery Sales

Tomlin Architectural Millwork

Tooling on the Web

Toolstoday.com

Top Drawer

Touch Up Solutions LLC

Tractivity

TradeJobPlacement.com

TradeSoft

Trakware Systems Inc.

TRB Flooring Company

Tropical Hardwoods

True North Cedar

Ubidmachinery Inc.

UC Coatings Corp.

Unique Building Supples

Unique Machine & Tool

University of Wisconsin

UWMO Auctions

VacDry Kilns

Vacuum Pressing Systems, Inc.

Vacuumpods.com

Valspar

Vecoplan LLC

Vector Art 3D

Vectric Ltd.

Veneer Systems Inc.




Cottonwood for horse stalls       Is this a suitable species? September 25, 2002

Question
A customer wants me to saw some lumber for horse stalls. He has a lot of large eastern cottonwood trees that he has been told would be suitable. I am a little concerned that the cottonwood might be too soft. He also has water oak and hickory.

Forum Responses
Cottonwood is the choice of champions. Cottonwood does not sliver and therefore, many breeders use it as flooring. After it has dried, try driving a nail into it.



I agree. No slivers and horse pee seems to make cottonwood as tough as steel. Once when I was camping, I gave a dry piece the ole Paul Bunion with a good axe. I ended up throwing the cottonwood, axe and all into the fire cause there was no way to get the axe head (broke the handle off) out of the wood.


They won't chew on it, either. It will work much better than the water oak or hickory.


Saw it and nail it as quick as you can. There are several old buildings including a barn here made from cottonwood that have been around close to 100 years, so I am told by the old timers. I sawed some standing dead cottonwood earlier this summer for corrals. We put two coats of good paint on it. I wonder how it will hold up outside. Time will tell.


If you do not have white oak, the cottonwood is best. Hickory will rot if wet and bugs will eat it up. Water oak is a red oak and will not hold up well if in ground contact or wet. If you are using them for posts in the ground, put in some bug dope or some other environmentally unfriendly stuff to help with the life of the post.


I cut a lot of lumber for horse stalls and the most requested and used is red oak, due to the fact that horses won't chew it. It is very bitter and doesn't have a pleasant smell to them. I have never used cottonwood, so I can't give advice on that, but I have used pine, pecan, sweetgum and poplar and all were eaten by bored horses in a stall. I have seen horses that are bored or upset in a stall eat a 2 X 12 board plum into pieces in less than a day's time. My vet tells me that red oak is poisonous to them, but since they won't even try to chew on it, they will never get enough of it to hurt them.


You could mix lumber types, yes? Some people around here use pine, but I'm currently writing doctors to have their heads examined for tumors. At minimum, cottonwood for the top "rail" or plank.

From what I have seen, Eastern cottonwood does not hold up well at all when outdoors. The wet/dry/rewet cycle just rots the snot out of it. It is true that is dries like steel. If I ever have to split a piece of cottonwood that has dried, I just install a ripping chain on my saw and have at it.



Interesting with the horse stable thing. What is the Latin name for cottonwood? I've never heard that name connected with a European species.


In my area of southwest B.C., it is Black Cottonwood (Populus balsamifera trichocarpa), used mainly as pulp. But I have seen it used as panels on a custom door and as trim. It had a pretty colour that caught my eye, and when I asked, I was surprised to find out what it was.

A lowbed operator had some cut as planking for the bed, but told me it busted up too fast. I wonder if it should have dried, as it was green and used right away?



Eastern cottonwood is Populus deltoides. One interesting point is that the carvers really go for the bark. The bark of old and usually big trees gets deeply etched and some woodcarvers like to do faces on it. I don't know how you would go about harvesting it to be in good enough condition for resale, but the dried bark goes for $5.00/lb. US or about $7.50-8.00 CDN for 2.2 kilos.

And if you have ever tried to split a piece of elm with the grain that corkscrews down the piece, you will have some fun.



The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor A:
The only oak that our horses don't crib chew is blackjack, but like all oak that is in contact with the ground, it rots easily.

I used some cottonwood inside for stall walls and that above the soil level has lasted well (16 years).

But the king of wood for stalls is persimmon - it is wonderful, hard and long lasting. I had cut one very large persimmon from our Oklahoma farm and it made the best stalls in the barn.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Primary Processing: General

  • KnowledgeBase: Wood Engineering

  • KnowledgeBase: Wood Engineering: Wood Properties

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article