Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Creating a Heavy Laminated Furniture Frame       A furniture maker gets tips on wood bending and lamination for a four-by-four curved hammock-chair frame. May 23, 2007

Question
We would like to produce a hammock chair stand, and feel that a bent lamination method might work for us. We have produced two forms (one male, one female) to be used as a press. The radius of the curve to be produced is 27'' inside, 31" outside. To eliminate as much of the trial and error as possible, I've read every thread on bending and laminating on this site. I'm still somewhat confused. If I use laminating strips of 1/4" in thickness x 4" in width, will I need to steam, bend, dry and finally laminate? Or will that thickness bend to my radius without steam? Perhaps a thinner thickness would work better? Should I use dry wood or green? Finally, with regard to lumber selection, I would like to use oak as it appears to be a good choice for bending, has a nice appearance when finished, and is strong (stand will need to hold 250 lbs). Is there a particular grade of lumber I need specify? And is there an industry term for surfaced laminating strips?

Forum Responses
(Furniture Making Forum)
From contributor J:
Run some tests - if the unsteamed pieces bend without breaking, then steaming isn't necessary. If they break, then try using thinner pieces. If the radius is very tight and the laminations are as thin as you wish to saw them, and they still break, then steaming may be required.

Ash and oak are good bending woods. The wood should be dry. If you use green wood, it will dry eventually, and the results will be uncontrolled. If the joint is stressed and the wood has drying defects in it, then there could be some strength issues.



From contributor K:
That sounds like a vacuum bagging job to me. I have not used a two part form since learning it about 20 years ago. I would drop on down to 3/16", and use a thickened epoxy, then slip them into a bag. Use only enough clamps to hold the parts to the form, then draw the vacuum. Spread some epoxy onto a scrap to monitor how long it takes to kick by feel.


From contributor B:
How thick is your final product after glue up? If it is 3/4", then 1/4" thick strips will only allow 3 strips. This won't be enough to even begin to prevent springback without a pre-steam bending step.


From contributor C:
If I follow correctly, these arcs will be sections of a circle with sixteen plies and be about 4" by 4". If this is right, your forms or cauls should be very heavily built to withstand a lot of bar clamps without coming apart or deforming. With this type of laminate, it should not be necessary to steam the boards. How much of a circle are these pieces when done?


From contributor B:
I should have read your post a second time. It does seem you indicate a 4" final part thickness. Our experience with thick laminations is that they tend to spring in versus out. This is probably due to the absorption of moisture from water based glues on thinner strips. I would suggest 1/4" strips and think you should be able to do this without pre-steam bending the parts. At 4" final thickness, you should get almost no springback.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Furniture

  • KnowledgeBase: Furniture: General

  • KnowledgeBase: Woodworking Miscellaneous

  • KnowledgeBase: Woodworking Miscellaneous: Bending Wood




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.