Today's
Sponsors:


Veneer Systems Inc.

Vintage Wood Products

VortexTool Co. Inc.

VyTek

W. Moore Profiles, Ltd.

Wagner Electronic Products

WalzCraft Industries

WEIMA America, Inc.

Weinig

Western Dovetail

Williams and Hussey

Wisconsin Knife Works

WiseWood Veneer

Wizard Industries

WMMA

Wood Doctor's Rx, LLC

Wood Source

Wood Technology Inc

Wood-Mizer

WoodCabinetDoors.com

WoodenBoat

WoodJobs.com Search Consultants

WoodLINKS

Woodmaster

WoodPlanet Inc.

WoodSprayGuns.com

WOODWEB

Woodworker's Supply/woodworker.com

Woodworker's Directory

Woodworking Network, a Division of Vance Corporation

Woodworking Technology

Wright Timber

Zipbolt

T-Tool USA LLC

Taghkanic CNC Services

TaylorCraft Cabinet Door Company

Techno CNC Routers

Template Services

Terminus

The Machine Warehouse

Thermwood Corporation

TigerStop

TigerwoodDecking.com

TimberKing

TimberTop Woods

Timesavers Inc.

TMS Machinery Sales

Tooling on the Web

Touch Up Solutions

Tractivity

TradeJobPlacement.com

TradeSoft

Tritec/GANNOmat

Tropical Hardwoods

TSI

UC Coatings Corp.

Unique Building Supples

Unique Machine & Tool

University of Wisconsin

Urban Evolutions

UWMO Auctions

Vacuum Pressing Systems, Inc.

Vacuumpods.com

Valspar

Vectric Ltd.




Diameter Growth Models Using Minnesota Forest Inventory and Analysis Data

      The Forest Inventory and Analysis (FIA) program of the USDA Forest Service North Central Research Station (NCRS) has begun replacing the 12-to 13-yr periodic inventory cycles for the states in the North Central region with annual inventories featuring measurement of approximately 20% of all plots in each of the 11 states each year. State reports on summaries of the forest resources will be produced every 5 yr. As a method of updating information on plots not visited in the current year, NCRS is developing nonlinear, individual-tree, distance-independent annual diameter growth models for species groups. The models, formulated as the product of an average diameter growth component and a modifier component, were calibrated on Minnesota FIA data from stands that were generally,undisturbed, of mixed ages and of mixed species. The dependent variable is annual diameter growth. The independent variables include crown ratio, crown class, stand basal area, stand basal area larger,than the subject tree, physiographic class, and latitude and longitude of plot locations. The model predictions at both the individual-tree level and plot level have negligible bias, and the models may be easily recalibrated to include new data sets obtained from the annual inventories. 2001 This article is in PDF format (file size: 1858 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Diameter Growth Models Using Minnesota Forest Inventory and Analysis Data   (2001)

The Forest Inventory and Analysis (FIA) program of the USDA Forest Service North Central Research Station (NCRS) has begun replacing the 12-to 13-yr periodic inventory cycles for the states in the North Central region with annual inventories featuring measurement of approximately 20% of all plots in each of the 11 states each year. State reports on summaries of the forest resources will be produced every 5 yr. As a method of updating information on plots not visited in the current year, NCRS is developing nonlinear, individual-tree, distance-independent annual diameter growth models for species groups. The models, formulated as the product of an average diameter growth component and a modifier component, were calibrated on Minnesota FIA data from stands that were generally,undisturbed, of mixed ages and of mixed species. The dependent variable is annual diameter growth. The independent variables include crown ratio, crown class, stand basal area, stand basal area larger,than the subject tree, physiographic class, and latitude and longitude of plot locations. The model predictions at both the individual-tree level and plot level have negligible bias, and the models may be easily recalibrated to include new data sets obtained from the annual inventories.

Author: Lessard, Veronica C.; McRoberts, Ronald E.; Holdaway, Margaret R.

Source: Forest Science. Vol. 47 no. 3.:p. 301-310. (2001)

Citation: Lessard, Veronica C.; McRoberts, Ronald E.; Holdaway, Margaret R.  2001.  Diameter Growth Models Using Minnesota Forest Inventory and Analysis Data  Forest Science. Vol. 47 no. 3.:p. 301-310. (2001).

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: FPL (Forest Products Laboratory)

  • KnowledgeBase: Forestry

  • KnowledgeBase: FPL (Forest Products Laboratory)




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2012 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article