Question
Has anybody used FastCap's 2P-10 glue, which is supposed to bond in 10 seconds? I was thinking about using it for crown mold so that I could get nice square corners without nail holes to fill.

Forum Responses
(Adhesive Forum)
From contributor D:
I use miter bond, which is essentially the same thing. It works great - I love the stuff.



From contributor B:
The process is da bomb, regardless of manufacturer. There’s a bit of a learning curve - how much glue/accelerator for various materials (like anything else). It's a bit expensive, but definitely ups the quality, and saves time. I wouldn’t go into a trim job or an install without it. I use it in the shop, too, for quick repairs of splinters and small splits. Dang strong, too.


From the original questioner:
What are the names of this glue and who sells it? Sounds great for crown!


From contributor G:
You can find the FastCap 2p-10 glue on Amazon and a few other online stores. One out of PA is cdmcabinethardware.com. Also check out the FastCap website to find retailers in your state. The glue works great!


From the original questioner:
Thanks for all the info! I hate crown, but seem to get so much of it lately. This should make it a little more bearable. I always get pre-finished crown and it's very tedious work.


From contributor K:
Just got my 2P-10 kit yesterday and happened to have a kitchen to crown today. The 4" crown was pre-finished cherry with a glaze, which doesn't look good with any filler. Great stuff! Really don't know what I was thinking before the 2P-10. I bought the kit with the medium, heavy, jel, debonder and activator for $36. I thought it was pricey for some super glue, but it paid for itself just today, and a perfect job.

On one section that wrapped around a corner, 7 feet by 7 feet (outside corner), I glued up the two pieces before putting them up. I had this 7x7 "L" of crown sitting on the counter. I also had my 23 ga pinner on the same counter. The other installer caught the air hose with his foot. The glued-up piece crashed to the tiled floor, but the corner held perfect. Truly strong bond in seconds.

The photo is a 1x5 of poplar I glued up tonight (about 3/4" overlap). I tried pulling it apart after 20 seconds and couldn't. I then pushed down on a table and had my wife push the other end. Snapped the wood but not the bond! It will change the way I work.




From contributor K:
Where it snapped... When I went to knock that remaining piece off again with a hammer, about 1/2 the joint held again and took off more splinters. I'm sold.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Adhesives, Gluing and Laminating

  • KnowledgeBase: Architectural Millwork

  • KnowledgeBase: Architectural Millwork: Millwork Installer


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2020 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article