Today's
Sponsors:


Vintage Wood Products

VortexTool Co. Inc.

VyTek

W. Moore Profiles, Ltd.

W.L. Fuller

Wagner Electronic Products

WalzCraft Industries

WEIMA America, Inc.

Weinig Group - USA

Western Dovetail

Williams and Hussey

Wisconsin Knife Works

WMIA

WMMA

Wood Doctor's Rx, LLC

Wood Technology Inc

Wood-Mizer

WoodCabinetDoors.Com

WoodenBoat

WoodFinder

WoodJobs.com Search Consultants

WoodLINKS

Woodmaster

WoodPlanet Inc.

WoodSprayGuns.com

WOODWEB

Woodworker's Supply/woodworker.com

Woodworker's Directory

Woodworking in America

Wright Timber

Specialtytools.com

Speed Sander

Spink Lumber

Sprayguncaptain.com

Stefani

Steve H. Wall Lumber Co.

Stiles Machinery

Stiles Shop Solutions

Stoneys Hardwoods

Super Source Tooling Inc.

Supergrit Abrasives

Superior Wood Products

T-Tool USA LLC

Target Coatings

TaylorCraft Cabinet Door Company

Techno CNC Routers

Template Services

The Veneer Store

Thermwood Corporation

Tiger Wood Ltd.

TigerStop

TigerwoodDecking.com

TimberKing

Timesavers Inc.

TMS Machinery Sales

Tomlin Architectural Millwork

Tooling on the Web

Toolstoday.com

Top Drawer

Touch Up Solutions LLC

Tractivity

TradeJobPlacement.com

TradeSoft

Trakware Systems Inc.

TRB Flooring Company

Tropical Hardwoods

True North Cedar

Ubidmachinery Inc.

UC Coatings Corp.

Unique Building Supples

Unique Machine & Tool

University of Wisconsin

UWMO Auctions

VacDry Kilns

Vacuum Pressing Systems, Inc.

Vacuumpods.com

Valspar

Vecoplan LLC

Vector Art 3D

Vectric Ltd.

Veneer Systems Inc.




Flat Panel Door Material       for the job? February 25, 2005

Question
I have an order to replace about 30 cabinet doors with a five-piece, flat panel door. The doors will be painted white by the customer. I will be using birch for the rails and stiles, but am looking for feedback on the panel. I'm not thrilled with 1/4" panels. Seems cheap to me. Would 1/2" MDF run through the shaper to achieve my 1/4" tongue be too heavy? I'm looking for any ideas on a good paint grade panel. If 1/4" is okay, I would like to hear that as well.

Forum Responses
(Cabinetmaking Forum)
I don't do 1/4" either, so I use 1/2" MDF. I prefer maple for the stiles and rails. Most shops near me use 1/4" with no apparent problems, though.



What would the customer want? If it's only a paint grade door, than 1/4" should be fine. If the customer wants to pay more for a 1/2" panel, then go that route. I would use 1/2" birch veneer over MDF and your slot cutter to remove 1/4" of material so it could slide into your rails. Just leave the heavy side to the back of the door so you don't lose the reveal on the front side.


The 1/4" veneered plywood I have been getting is barely 3/16", so it will cause hassles with your 1/4" slot. If you are suggesting getting a birch veneer on an MDF substrate, why bother with the extra cost of the veneer if it will just get painted?

MDF will run through your shaper well, but it is hard on your cutters. I don't think it will be too heavy for your doors. It will cause you extra sanding to get rid of the hairs on the part you shaped, though. As long as the customer isn't planning on trying to put his fist through the doors, I don't see anything wrong with using the 1/4" panels. MDF is stronger than particleboard and weighs about the same, and MDF is designed to be painted.



I make my doors from ash veneered MDF. Stiles and rails are 3/4", centre panel 1/4". I use the ash veneered stuff because I paint with water based acrylic paint, and it tends to raise the grain of plain MDF. I know MDF doesn't have grain, but surface is definitely affected by water based paint. I don't care for the smell of other types. The other advantage to the veneer is that the grain shows through the paint and the customers find that attractive.

The 1/4 inch centre panel looks fine and makes the door a little lighter, which affects the feel as the door is opened and closed.



My thoughts, exactly. You beat me to the punch. If you're going to use solid MDF for your field, you might as well use it for your rails and stiles. Then you will have a heavy door, if that's what you're after.


Use 1/2 MDF and back cutter to get the 1/4 for rails and stiles.


I think you all forgot something! What about 3/8" MDF? Seems to be a perfect solution...


The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor J:
I agree with the 3/8" MDF suggestion, although I just finished two paint grade jobs using 1/4" hardboard. It takes primer great and is durable and inexpensive. I would leave MDF alone as far as the rails and stiles are concerned. I use poplar or, depending on intended use, soft maple. Real world usage (especially if your clients have children!) would leave MDF in pieces over time, where solid wood will hold up better.



Comment from contributor G:
I use the (undersized) 1/4" panels for my doors, but I also fit an additional panel on the back (inside) of the door. It makes the door feel more substantial, while not increasing the weight significantly.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: Commercial Cabinetry

  • KnowledgeBase: Cabinetmaking: Custom Cabinet Construction

  • KnowledgeBase: Cabinetmaking: Cabinet Design

  • KnowledgeBase: Cabinetmaking: Cabinet Door Construction

  • KnowledgeBase: Cabinetmaking: General

  • KnowledgeBase: Cabinetmaking: Residential Cabinetry

  • KnowledgeBase: Cabinetmaking: Store Fixtures

  • KnowledgeBase: Woodworking Miscellaneous

  • KnowledgeBase: Woodworking Miscellaneous: Woodworking




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article