Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




Glues Interfering With Water-Borne Stain on Veneer       Advice on fixing a problem where glued veneer seams telegraph through water-borne stain finishes. June 9, 2007

Question
I have recently begun using water based stain in our finish shop. The variation in colors and consistency of stain is great. However, when going over certain veneer, the seams become apparent. Are there certain types of glue that should or should not be used when laying up veneer, when water-borne stains are being applied? What should I suggest to millwork providers?

Forum Responses
(Veneer Forum)
From contributor D:
Which veneers are the seams visible in?



From the original questioner:
So far, both on birch and maple.


From John Van Brussel, forum technical advisor:
Water based stains and veneers are not a good mix. What do you mean by you see the seams?


From the original questioner:
I'm beginning to find out that waterbased stains and veneers are not a good fit. However, with VOC demands and the push for "green" building in commercial and now residential in the NW, we are going to have to find some way of working together to make it a good mix, or someone is going to suffer in the end. There must be some sort of adhesive that is more water stain friendly…. isn't there? What I mean by seams is, where two skins are laid up side by side, the seam between them turns light compared to the wood itself. I'm assuming that is where adhesive has squeezed out and not been totally sanded away.


From John Van Brussel, forum technical advisor:
My guess is the veneers were spliced with a PVA glue which will not accept stain, water based or solvent based. You will need to get faces that have been zigzagged or taped or urea glue spliced.


From contributor J:
One way to prevent any problems would be to spray a seal coat on the panel first, then apply the stain. This process does multiple things: prevents blotching, some barber-poling, etc., and will aid in solving your problem as well.


From contributor T:
Try spraying on a wb dye stain like Fuhr 155, but mist it on very lightly. Test your spray setup on sheets of paper first. You want a real light mist so it dries instantly. Then keep going over your work one coat after another until it is the right darkness. Each coat must dry a minute or so. Don't soak the wood. Your first clear coat should also be light so it dries fast too. Once you get it sealed, you can go heavy. Practice on some sample boards. If it isn't dark enough, just mist on more stain between top coats. I like Fuhr 255 or Chemcraft's acrylic wb. All I use are wb. and I love it. Fast, clean, and beautiful.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing

  • KnowledgeBase: Veneer

  • KnowledgeBase: Veneer: Techniques




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article