Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Gluing Wood Flooring to Concrete       Adhesive choices for glue-down wood strip flooring. July 12, 2008

Question
I have been asked by a client to install wood floors in a few antique passenger train cars. The existing floor is a concrete slab. The train cars will be in use June through October every year. So far I think floating an engineered hardwood floor, over a Floor Muffler type underlayment. As far as glue for the tongue and groove, should I use polyvinyl acetate, or aliphatic resin? Would using a PVA be better because of the excessive vibrations?

Forum Responses
(Architectural Woodworking Forum)
From Professor Gene Wengert, Sawing and Drying Forum technical advisor:
Why would you want to glue the t&g flooring? If you do glue, avoid poly-vinyl acetate (PVA) even if it is an aliphatic resin type. You need something that is more flexible and will resist heat and moisture (I suspect). I would consider PL-400. For underlayment, will it be getting damp or wet? The traditional product for freight cars was white oak. Why not consider flooring similar to what is used in 18-wheelers today?



From contributor G:
How authentic do you want to be? Twenty or more years ago when the BC rail cars changed over to nailable metal floors and discarded the old flooring in our local dump, I brought lots of them home for garden boxes. They were maple, if I recall correctly, and made of strips bolted through and through with huge bolts. No glue involved.


From contributor D:
Wood flooring can be full trowel glued with products made specifically for that purpose. For commercial use I recommend SLC 3000 by Rinaldi, Italian glue that is elastomeric so wood can expand and contract seasonally without delamination. 3M Tartan brand strap tape can be used to hold planks together while glue cures. The green tack of the SLC adhesive is strong enough that no weighting or down pressure is required.


From the original questioner:
Thanks for all the advice. I am now going to go the solid white oak route instead of engineered hardwood. More authentic and a much better look. It was my first thought, but I just didn't think it would work. Since the slab is totally dry with no chance of moisture, I plan to glue straight to the surface after priming. SLC Silovil L38 looks perfect. A comparable adhesive I found was SikaBond T55. It is recommended to use in conjunction with Sika Primer. They also have an interesting Sika AcouBond-System that uses a slotted foam mat as acoustical dampening. The slots get filled with glue so the wood floor is directly glued to the slab. Looks too good to be true. Has anyone used this product?


From contributor D:
Sika makes a good product and they have been around for a while. The cleanup is much more difficult than SLC and the Sika also has a strong solvent smell, unlike SLC, which has a mild urea odor. Sika is single component and has a wide range of cure time r/t environmental conditions. SLC is a 2 component and cures much more reliably. Both are excellent products.


The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor J:
I have used the Sikabond system. It is excellent for gluing flooring to concrete. The slotted system is used with engineered flooring. Just understand that solid flooring will expand and shrink more than nailed down systems. You will have better results with shorter boards in length, no longer than 3' and widths no wider than 3 1/4". You may also have to clamp the flooring with straps to pull boards tight together.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Adhesives, Gluing and Laminating

  • KnowledgeBase: Adhesives, Gluing and Laminating: Glues and Bonding Agents

  • KnowledgeBase: Architectural Millwork

  • KnowledgeBase: Architectural Millwork: Flooring




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article