Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




Hand Clamping for Mitered Doors       What's a simple shop setup for assembling mitered cabinet doors? Pros supply a beginner with tips and suggestions. July 25, 2005

Question
I am looking for some advice on building mitered doors and frames. I've worked for a big furniture manufacturer for years, and we mitered stock on a Bell 424A which bored for dowels at the same time. Then we assembled the frames on a Lancaster air clamp. A little glue, some senclamps for good measure and off they went.

Now, I'm trying to build the better mousetrap in my own shop. I can miter ok with my miter saw and a little sanding. I've read plenty of posts on that. My problem is assembling the frames. I have a couple band clamps but they don’t work well.

Does anyone have any ideas on an economical solution that gives a quality result? I usually work with oak, pine, poplar, and mahogany, and the widest mouldings I've fooled with have been about 3", and frame sizes from 6 X 6 up to around 24 X 36. I’m not looking for high production - just a way to build and set the frames off for the glue to dry. I have even used biscuits on a few larger frames, but still had a problem keeping everything clamped tight.

I do have an old Senclamp gun, but it just doesn't do its job unless I have solid pressure on the joint. And on pine, it's just fairly useless - the nails just crush the softwoods. I hope the pros take it easy on me. I thought I had all the answers until I realized my equipment doesn't compare to the multi-thousand dollar equipment I had experience on. But, like anything worth doing, there's a lot to learn and a lot to be gained.

Forum Responses
(Furniture Making Forum)
From contributor P:
It is possible to glue up mitered frame with regular Jorgenson lightweight bar clamps, but there is a trick to it. Start by applying glue to joints and closing all four as well as possible by hand. Lay the frame on a flat surface. Put two clamps parallel to each other and tighten until the pads barely make contact with the wood. Rotate the clamp bars until they are flat against the frame. Then put two other clamps running 90 degrees to them, so that their bars are resting on the bars of the other clamps, and also tighten until they are barely closed.

At this point you have four clamps on the frame. The handles of both pairs of clamps should be on adjacent sides, the dead ends on the opposite adjacent sides. Now slowly tighten the two handles in on corner a turn, then the two handles that are not next to each other, back and forth, until the miters close. (This whole procedure is much harder to describe with words than to show you.) You have to watch carefully to make sure that the frames are in alignment as you tighten the joints - it is very difficult to adjust this while the clamps are tightening.

But if you positioned the frames correctly before tightening, the whole thing will close up very nicely. Also, you have to cut perfect 45 degree miters also. I have done this many times making picture frames for my wife, and it is quite fast and works well if you are careful. I use biscuits of splines when I am doing this. You might want to practice on scrap before doing this for keeps.

I would forget strap clamps – they don’t work well. You might also want to make a clamping frame two fences at 90 degrees, an open corner where the fences would meet, and an open bar back to support the glue ups - then you can clamp two sides of the frame to the fences, and it should square the frame and close the joints. With miters, perfect 45s and stock of consistent flatness and width make everything a lot easier.



From contributor J:
Here are the clamps that I like to use. These clamps are great for all sorts of tough situations.

Gross Stabil Mitre Clamps
http://www.woodessence.com/GrossStabildefault.html



From contributor G:
Years ago I had a friend that had a machine shop. I had him machine four 2"x2" L shaped blocks with one end to accept a 3/8" threaded rod. In the opposite side of the L shape block had a through hole to let the 3/8" threaded slip through. This clamp allows for any size clamp up from about 4 inches to the length of the threaded rod and at the same time squares the frame. It has worked very well for me and is very quick. There are clamps available like this from woodworking tool suppliers. They are usually made from plastic and 1/4 inch threaded rod which is ok if you do not need to apply much pressure to the corners.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: Cabinet Door Construction




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article