Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




How did our forebears dry lumber?       How lumber was dried for furniture construction prior to the introduction of kiln drying. November 21, 2000

Question
How did the 18th century furniture makers build such beautiful furniture if they only had access to air dried lumber? Unless I'm wrong, and please tell me if I am, I don't believe they had kilns to dry their lumber to a 6%-8% MC. Didn't they use the same 10%-14% air dried lumber that us do-it-yourselfers use today?

If not, what did they do differently that we can't do today? And are we really going to encounter problems with air dried lumber as many people indicate we will? Maybe the old timers air dried their lumber first and then brought it into their working environment for a sufficient period of time to acclimate the wood before using it. Maybe this made the difference. Anyone have any historical information on this?

Forum Responses
I've read that in the old days wood craftsmen would air dry their lumber in open sided barns for many months just as we do now days in air drying. Once the wood had dried out enough they would bring it inside their workshops or homes and keep it close to a hearth or stove when in use to draw out the rest of the moisture (many more months). They say that you could tell when it was ready by the sound made when you knocked on it.



I think that the main reason air dried lumber worked in the 18th century is because of the lack of air conditioning and heating. So, most likely the homes probably had conditions close to the conditions the lumber dried in to begin with.

I'm by no means a carpenter, but I couldn't see myself putting all this time and craftsmanship into a piece of furniture only to watch it go unsquare and develop cracks in the joints.



The last theory is correct--in earlier times the lack of what we would consider adequate heating and cooling played a big role in not only the necessary moisture content, but also in the design. The air exchange in a current day home is almost nil as compared to one from prior centuries, and when coupled with humidifiers and dehumidifiers, we enjoy far greater stability in humidity and temperature.

Air exchange would be responsible for greater swings in moisture content especially season to season, as well as a higher MC in winter months because of moisture being able to enter the living space more readily. Because of this, their designs had to be capable of adjusting to a greater range of humidities. A more recent example of this would be wooden single pane windows. They were difficult to operate in the summer because of swelling due to higher humidities and drafty and loose fitting in the winter due to reduced humidities because of heating.

Winter typically sets the low MC requirement because air that is cold is denser (let's say compressed) and when heated it expands (decompressing), creating a greater volume: the water molecules in the air are now spread out over a greater volume and thus the amount of water present in a given volume of air is less than it was before it was heated, hence the term relative humidity. Also, there is greater area between the air molecules allowing more water to be held.

The real key to remember in drying is balance. The moisture content in the wood must balance with that of the air, neither gaining nor losing any significant amount of moisture. Fortunately, the wood will reach that balance for us. Unfortunately, its time table doesn't usually fit into ours, thus requiring kilns to create artificial conditions that don't normally exist year round (extremely high temperatures with extremely low humidities), allowing us not only to dry wood faster, but to be able to acheive MC levels comparable to those only found in winter months.

If you lived in a greenhouse "dry" would be quite different compared to the desert Southwest. All that is required is balance, not a magical number or percentage, to have functional wood.

You can reach the same MCs as kiln dried wood by air drying--it is merely a function of time and conditions (and sweat).



The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor J:
There are several other factors:
Wood was winter cut. Wood was stored for long periods of time, up to 1 year for 2X material. The wood industry was geared for long air drying so, logging, storage, and useage were complimentary. Primary cut timber and second growth timber have vast amounts of moisture difference.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Primary Processing: Air Drying Lumber

  • KnowledgeBase: Primary Processing: Kiln Operation

  • KnowledgeBase: Woodworking Miscellaneous: Woodworking

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article