How to Determine Polyetheylene Glycol 1,000 Content in Treated Wood
An experimental technique using water extraction for evaluation of the content of ployethylene glycol of molecular weight 1,000 in wood where the ovendry weight of the untreated wood is not available was shown to be applicable for PEG-treated black oak and yellow-poplar. 1975
This article is in PDF format (file size: 825 kb).
To download this article, right click on the link immediately below
and choose "save target as". To view the article, left click the link
immediately below. (Download the latest
Acrobat Reader if required.)
How to Determine Polyetheylene Glycol 1,000 Content in Treated Wood (1975)
An experimental technique using water extraction for evaluation of the content of ployethylene glycol of molecular weight 1,000 in wood where the ovendry weight of the untreated wood is not available was shown to be applicable for PEG-treated black oak and yellow-poplar.
Author: Rosen, Howard N.
Source: Research Note NC-191. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station
Citation: Rosen, Howard N. 1975. How to Determine Polyetheylene Glycol 1,000 Content in Treated Wood Research Note NC-191. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station.
Would you like to add information to this article? Interested in writing or submitting an article? Have a question about this article?
Have you reviewed the related Knowledge Base areas below? KnowledgeBase: FPL (Forest Products Laboratory)

KnowledgeBase: Forestry

KnowledgeBase: FPL (Forest Products Laboratory)

Would you like to add information to this article? ...
Click Here
If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to review our Forum Guidelines.
Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.
When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.
Return to beginning of article.
|