Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Identifying Black Locust       A woodturner tries to figure out if the wood he's using is Black Locust. February 15, 2009

Question
I have been turning a log left from highway clearing. The leaves and branches have been ground so I can't use them for identification. At first glance I thought the wood was butternut, due to the deeply furrowed bark, but it quickly became apparent by the hardness that it was something else. There was not much of a distinguishing odor to the lumber, but one thing I noticed and that the forum on locust didn't mention was that the wood was even worse than walnut in the way that it stained my hands a dark black/blue. Does anyone have any ideas?

Forum Responses
(Sawing and Drying Forum)
From the original questioner:
I forgot to mention that the wood was from central Connecticut.



From contributor L:
Can you post an image? What color is it when freshly cut?


From contributor M:
Black locust has a light yellow color off the mill. The color is a deeper yellow when black locust is kiln dried.


From Gene Wengert, forum technical advisor:
Do you have a "black light" source? Locust will fluoresce when exposed to UV.


From contributor R:
Locust smells. Once you cut it you'll never forget it. Minimal sapwood on black locust. I'm in CT as well and mill it quite often. As for staining your hands it’s not as bad as walnut or butternut. Maybe you do have butternut. A butternut log would be light weight compared to black locust. There are not too many physical similarities between the two.


From the original questioner:
I turned another bowl yesterday, and am beginning to think that it is definitely black locust. When first cut it was a light yellow, with greenish tinge, and it quickly started to oxidize into a deep gold/light tan. The tree was about 18" in diameter and had a somewhat pronounced darker heart of about 6" in diameter. The odor was nothing like butternut, of which I dislike greatly. Instead, it had a sort of sweet, cut grass or fresh grain aroma. The bark was very deeply furrowed, and almost resembled cork for 1/2", although it was quite stringy. Again, I mention the staining. The white sealing wax I use almost immediately started to turn brown on contact with the wood. The wood seems to be quite stable, with minimal checking. I've roughed maybe twenty five bowls ranging in diameter from 8 to 16 inches out of the tree, and am looking forward to completing them when dry, no matter what the species.


From contributor T:
Butternut tends to have a very shallow furrow in the bark, and without the furrow, the flatter parts would resemble something like ailanthus. Black locust does have very deep furrows unless the tree is young.

It sounds like you have black locust. You seem to have described the strong smell as freshly cut grass perfectly. It is also common for black locust to get a darker heart as it rots on the interior, as this wood is best harvested when young. Very few woods have a normal double heartwood with a different tone of color. Is there any difference in density in the darker hearwood? Stay away from the bark as it is toxic to animals. The toxicity to humans seems to be unknown.



From contributor W:
If it is black locust, there will only be a few rings of sapwood, the rest will be heartwood. If that is not the case, it is not black locust. What you described sounds like it could also be mulberry.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Lumber & Plywood: Wood Identification




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.