Installing a Kitchen Island over Tile

      How to attach a cabinet base to a tile floor. July 2, 2008

How do you install an island over tile without destroying the tile? The customers do not want me to drill or remove anything. Can I glue it down? If I was to glue it down, what could I use?

Forum Responses
(Cabinet and Millwork Installation Forum)
From contributor D:
If you can't drill through the tile maybe you could drill into a grout line at a place where four tiles come together, then anchor some blocking to screw the cabinet to. Some liquid nails under the blocking would also help.

From contributor F:
You can glue it down. I have build a frame under the cabs that are the right height, glued it to the floor and then screwed through the cabs down into the frame.

From the original questioner:
What type of glue?

From contributor L:
If your island has any weight to it at all you don't need much to hold it down. A light bead of silicone or pl glue should do it.

From contributor R:
Try polyurethane construction adhesive. Clean the tile first with alcohol or something similar.

From contributor J:
Sometimes the clients need to be educated on what can and cannot be done. Chances are any adhesive that is strong enough to firmly anchor an island will ruin the tiles it's attached to, whereas if you drill through the grout line it can always be filled at a later time.

Make sure it's ok to do this with local codes also. In my state any island which is secured must have electrical supply on it which would obviously mean drilling holes in the tiles.

From contributor K:
Screwing through the grout line is the way to go, but make sure they know the downfall if they remove the island (grout color difference, not only where the holes are, but the surrouding color variation box where the island was).

Other ways it's been done in clude:

1. Casters with locks (no fastener method).

2. Install 3-4 threaded pins in the grout line on one side (depending on size of island); drill a corresponding hole in the bottom of the island, and set in place.

3. Weighted base (no fastener method) - fabricate a separate to-kick box (complete box), which can have weights added to it on each corner, then attach rubber bumpers to the bottom, which won't slide on the tile. Position where the island will go, fill the box with weights (as much as you want, but be sure to secure whatever weights you use to the bottom or side of the toe-kick box), close the top (it's a box remember), then attached the island cabinet to the top of the toe-kick box. Attach finished kick material leaving a 1/6'-1/8" gap. The combination of the weights, bumpers, cabinet and countertop, along with the contents of the island and it's not going anywhere. Just make sure you charge for this.

There are other ways, but you get the picture. Personally, I would sell her on the idea of blocking screwed through the grout line. If she doesn't warm to that idea, propose the other alternatives above, at a premium, and she'll come around.

From contributor M:
Before you screw into the grout lines make sure there is no in-floor radiant heating. Glue it down with PL Premium or some other polyurethane glue.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: Installation

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article