Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Jointing knives of a side-head planer       Choosing and using the proper stone when jointing knives used in a side-head planer. November 7, 2000

Q.
We are currently running a Yates A20 planer 1962-66 with belt driven side heads. The heads are the 10 knife LVL model by BGR. What is the best way to joint these knives & what type of stone should I use?

A.
The type of tool steel and the spindle speed will determine the type of jointing stone. Also the accuracy of the grind must be known.

There are two types of jointing stones used today. They are the hard and soft stone styles. The soft stone works well for high rpm machines with accurate ground tooling. The hard stones work with tools that are hand ground and less accurate.

The stone must be shaped to fit into the tool. This shaping must be done before the stone is put into the holding bracket. The stone is then chipped in with the head and then pushed into the head while the head is at operational speed. This causes the removal of some metal off of each knive. This removal puts all the knives into the same cutting circle. Sparks can be created while doing this with both the hard and normal soft stones. There is a new non-sparking stone available from MSI that reduces the risk of fire. You can contact them at 704/528-3513.

Dave Rankin, forum technical advisor



From the original questioner:
How do you shape your stone to start with? Our sideheads run at 4200RPM and we grind the knives on a Reform flat bed grinder. The knives are initially set up on a stand and shaft assembly in combination with a dial indicator. We check both the radius & position of the side of the knife at this time. Any further suggestions?


In the MSI catalog there is a description on how to select and how to use jointing stones. This is a preveiw of usage. Also in "The Profiler", the Grinderman's Association newsletter additional information discusses the use of jointing stones. The Grinderman's can be reached at 704/528-3539.

Dave Rankin, forum technical advisor



From the original questioner:
We are running an early 60's Yates A20 Planer with belt driven side heads spinning at 4200 rpm. The right head sticks when we are trying to adjust for profiles. Upon investigation we found that this side runs 28-35 degrees warmer than the other side. We've changed bearings top and bottom, cleaned and polished all housings where they mate together, run grease recommended by Yates, all to no avail. Has anybody else had this problem and what did you do?


Sticking of the adjustment usually indicates a build up of contamination. This occurs frequently. The only way to properly repair this is to take the system apart and clean up the slides. As for the temperature difference, this may be due to the motor pull. If this cutter is removing more material it will heat up more. It could also be the bearings or the lubricant. There are many new lubricants that are available. I use Tech's Choice grease. This grease is fortified with additives that become part of the metal bearing race. It provides the metal with a great reduction in heat.

Dave Rankin, forum technical advisor



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Solid Wood Machining: Setup and Maintenance

  • KnowledgeBase: Solid Wood Machining: Tooling

  • KnowledgeBase: Solid Wood Machining: Tool Grinding

  • KnowledgeBase: Woodworking Miscellaneous: Tool Maintenance

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article