Today's
Sponsors:


Mereen-Johnson Machine Company

Merritt Woodwork

MFG in Honduras

Micro Fence

Microvellum

Middle Valley Lumber

Mikron Woodworking Machinery

Mill Outlet

Minimax

Mirror Reflections

MLS Machinery USA, Inc.

MLS Machinery

Modern Woodworking Magazine

Moldingknives.com

Monarch Machinery

Morbidelli

Moulder Services

Moulder Techniques

Mountainside Wood Products

Multicam, Inc.

NAP Gladu

Nebraska Tool

NEMI

New England Kiln Drying Association

NexGen

Hoffmann Machine Company

Holz Her U.S. Inc.

Howard S. Twichell Co.

Hvalsoe Sawmill Ltd.

ICA North America

Icy Straits Lumber

IDM

Impact Search and Placement

Indiana Hardwoods

Industrial Air Solutions

Integra Precision Grinding and Manufacturing

InTrading

Invicta Woodworking Machines

IpeDepot.com

irsauctions.com

Italpresse

J & G Machinery

J and J Barn Wood

J&P Machines

J. Gibson McIlvain Company

Jiffytops

JIT Hardware Supplies, Inc.

JMHsoftware.com

John G. Weber Co.

Joos USA Inc.

KCD Software

Kerber Farms and Mill

Keystone Wood Specialties

Keytrix Data Systems

Kiln-direct.com

Kleiberit Adhesives USA, Inc.

Kreg Tool Company

Kremlin

Lacy Cypress Inc.

Langelier Lumber Ltd.

Leadermac USA

Lewis Lumber Products

Lignomat

Logosol

Lumber Resources

Lumber Smith

M.L. Campbell

MACHINEKING.com

Macoser, Inc.

Mahros

Maine Timber Works

Maine Woods Company

Mann and Parker Lumber Co.

Martin Lumber

MARTIN Woodworking Machines Corp.

Mastercam - CNC Software

Matthews Mill

Maya Positioning Equipment




Keeping track of blade sharpenings       Comparing notes on noting the service history of sawmill blades. July 4, 2000

Question
I have over 100 bandmill blades in various stages of sharpening: sharp ones, to-be-sharpened, in the mail, at the sharpening sevice, etc.

I tried at first to keep track of how many times a band had been sharpened but as things went on it became too confusing, and new blades got mixed up with old ones. Anyone out there got a clever way of keeping track of such things?

Forum Responses
My solution: Purchase tags with string on them at any office supply store. When new blades come out of the box, place a tag on the wire which comes with the band. On the tag, record (1) date of purchase, pitch and angle. When it needs sharpening or setting, record this as item (2).

Basically all you are doing is manually recording what has been done to the blade.



Use Re-Sharp from Woodmizer and they will replace a blade when it is junk and send you a new one. That way, you never have to worry about any blades, and can spend your time cutting. It's the cheapest way to go, when you factor in your time.


My sharpening service stamps my bands with my initials and a dot for
every sharpening, next to the weld. This way I can tell how many uses each band gets.

I tend to use older bands for smaller logs (less stress) and newer bands on those wider cuts. It's a bear to remove a broken band from a 20-inch cut, but to ease removal, I use an old broken piece of blade with the set hammered flat, remove the sawdust from the kerf, and then I back the broken band out.

To keep track of board feet cut, stamp a code number and keep a log book.



From the original questioner:
I was wondering if etching the blade would work. Would it wear off too soon? Etching pens are available through commercial supply houses like McMaster Carr.

When they stamp a blade, what type of stamp are they using? The tags would work, but having a blade numbered seems foolproof.



I number my blades with a stamp or engraver near the weld. I use 3x5 cards on a binder ring to keep my records, one card for each blade. I make columns for the date of use and the running time. I keep track of the hook angles, the set, and sharpening times for each blade. I store my blades under the bench my sharpener is mounted on. Each blade has its own shelf or bin. This seems to work out well for me.


I have a cheap old engraver I simply mark my blades with. Then I use different color tie wraps, black and clear, to separate out whether they are for use with hardwood or softwood.


I use an engraver. I put a mark on the blade after each sharpening. I set and sharpen after every four sharpenings. I use Woodmizer blades. I've tried all other kinds: Lennox is so-so; Sandvik made a good blade but you can't get them anymore; Timberwolf is an excellent blade, but expensive; Simonds broke a lot. I think Woodmizer is about the best for the price.


The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor A:
The man that sharpens my blades uses a prick punch mark next to the weld on the outside of the blade each time he sharpens it. When I see six or seven dots on the blade I will try to saw only the smaller logs with it. You can make one for yourself from a chainsaw file. Simply grind a point on the hard end and cut the tang off and grind it, leaving a domed top to strike with a small hammer.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Primary Processing: Sawmilling

  • KnowledgeBase: Woodworking Miscellaneous: Tool Maintenance

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article