Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




Kiln wall material and insulation       What to use when you're building your own kiln. January 21, 2002

Q.
I'm building a 12 x 16 x 12 high kiln. I have the structure but need to put in walls and insulation. Any advice on the material I should use?

Forum Responses
I wood-framed with fibreglass insulation and ended up struggling for a while with vapour barriers.

I ended up tacking up Krona. (Other products of this type are usually polyethylene, which softens too much in the heat.) At first I couldn't find a tape that would seal it in the kiln environment. The 3M rep found me the stuff, though. 8951 is a tape for masking powdercoat or something, but it sticks tenaciously to the polyester surface of Krona and is unaffected by the heat and humidity.

You can get a guy to come in and blow polyurethane, which insulates and is a barrier too, but it costs a whack of dough.

I should add that, after foil tape failed on the Krona, I tried the Peel & Seal that Nyle sells. It is a 40 mil aluminum-faced asphaltic rubber made for low-slope roofing and such. It fell off the Krona, too. (Softens in the heat and pulls away.) Maybe it would seal other materials, but not the smooth polyester of Krona.



Polyurethane may not be the cheapest insulation, but considering its high R-value, I think it is a good value. It's also cheaper than rebuilding kilns every few years because of leaky vapor barriers allowing moisture to get to framing.


I had some pretty good luck using Ice and Water Shield™ (bituthene) as a vapor barrier over EPS foam board. I used both the standard and the high-temperature versions (the HT is much costlier) and saw no real difference in durability over a year of operation at temperatures averaging 130-150 degrees(F).


Will the Ice and Water Shield™ (bituthene) not eat away at the EPS foam board? I would think the solvents would dissolve it?


The bituthene still holds today. It is installed over thermax as well and still holds on that, too. If the adhesive ate at the styro, the bond didn't fail.


I am working on setting up a Nyle 200 now. We used fiberglass between the studs, 1 inch foam board, 6 mil plastic sheet then 1 inch pine lumber (so far). I am working on the doors now.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Kiln Construction

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.