Question
I'm a contractor with various guys coming and going over the span of this 4 year custom house we're building. Several areas such as the window liners/casing were brushed with urethane. I've taken up lacquering the natural hardwoods. I've heard a lot about compatibility issues regarding lacquer/urethane. I'm not clear if I could spray light coats of lacquer over the urethane or there is a sealer/primer available to use. I'm using Campbell catalyzed lacquer over a generic urethane that was picked up at the paint store.

Forum Responses
(Finishing Forum)
From contributor M:
If you are talking about spraying lacquer over the polyurethane and the poly is well aged, you might be able to get away with it by spraying light well-thinned coats of the lacquer. However, the poly might lift. The safest thing to do is to use dewaxed shellac over the poly and then you can go to the lacquer without worry.



From contributor A:
I would assume that the aged oil based poly has good resistance to the lacquer thinner. You could take a rag dampened with lacquer thinner and test a section.


From the original questioner:
The urethane went on perhaps 6 months ago. I'll try the shellac idea. Can I spray this, and how long do I need to wait before going into lacquer? I suppose I'll need to sand it out again.


From contributor M:
You can spray waxless shellac as easy as anything. Get some denatured alcohol (shellac thinner) to thin it for spraying, but it is already fairly thin. The beauty of shellac is that it doesn't bite into anything and nothing bites into it. So it is great for isolating two finishes which would harm each other. But by this same token, the finish prior to it (poly, in your case) will have to be rubbed down a little to give the shellac a mechanical bond since the shellac won't bite into the poly for a chemical bond. Same thing goes for the prep on the lacquer over the shellac.


From contributor G:
Have you tried using vinyl sealer as a bridge between the poly and the lacquer? It works effectively when you go between any nitro lacquer and conversion catalyzed varnishes, or vice-versa.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2018 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article