I need to build a built-in shelving unit in a master closet. I've done these before by using biscuits to make 12" shelves. They turned out great but were a lot of work gluing, scraping, sanding, etc. My local yard has 12" MDF shelving in-stock with a bullnose edge that looks great and is very inexpensive ($1.05 /foot for 12' pieces). I was planning to use birch or oak plywood for the uprights and centers with dadoes to hold the MDF shelves.

Here's where I have some questions. Has anyone used MDF for uprights and centers for built-in's instead of plywood? Is glue and a few nails from my gun enough to keep the MDF shelving in place? I see a lot about the need to screw the MDF using confirmats.

If I can do this whole job out of MDF it will cost a lot less and paint up great. However, I don't want to compromise on quality.

Forum Responses
(Cabinetmaking Forum)
From contributor P:
Between the glue, nails and the painter caulking never had a problem and the quality is still there as well.

Click here for higher quality, full size image

From contributor R:
Personally I can't stand MDF because of the formaldehyde and how fine the dust is that it clogs filters and dust masks in a heartbeat. That aside. MDF is easily worked, finished takes paint well and is generally stiffer than plywood. Two coats of dewaxed shellac or vinyl based underbody if you are using lacquer on the cuts sanding with 220 and 320 between brings back the smoothness and gets rid of the "pilling" in minutes. I use countersunk 2" screws and fill them with formula 27, sanded flush they disappear. As long as you are not trying to cover a large span unsupported you should be fine and you are correct as far as the savings is concerned. At 1.05 per foot have you figured your cost of ripping sheets at the 12" and running them through the shaper with a bullnose knife yourself? At four pieces from a 4 x 12 sheet if you need the 12 feet if not go to an 8 footer. Also, if you do have to do a wide unsupported span shelf consider using a soft maple edge 1-1/2 inch wide biscuited to the edge of the shelf for support.

For basic closet built-ins it’s great. What are you talking for a sheet from your supplier? I am in the north east and I can get birch paint grade plywood for 34.00 a sheet. I haven't priced MDF for a while as I haven't had a call for it lately. Also makes a good substrate for veneer. Just keep in mind. MDF has very little structural strength so in cases where you need it consider a dado instead of biscuits or just screws.

From the original questioner:
Oak sheets go for $63 and Birch are $66 from my local yard. At $1.05/foot for 12 footers with the bullnose, it's a time a money saver. I agree that MDF is nasty stuff to work with. The less I have to cut it - the better. I have a small shop so I may opt to get the local guys to rip a sheet of MDF into 12" 8 footers to use as the uprights.

From contributor M:
MDF is a great structural material, contrary to what was stated earlier. It is stiffer than most plywood. Do this test: rip 4" or so wide strips of plywood, particle board, and MDF of the same thickness about 4' long and then try to break them in half. You'll see which is strongest.

What MDF doesn't have is good edge strength, that is, it splits easily at the edges from screws, etc. I have found, incidentally, that ultra-light MDF is better for this than the dense stuff. I guess it's because, having less density, there is less displacement of material at the edges when fasteners are inserted. It's like inserting a screw without drilling into pine as opposed to maple.

From the original questioner:
I finished the job. I built the shelves out of MDF using biscuits to join the shelves to the uprights and it came out very nice. The shelves weren't very long so flexing wasn't a problem. It painted well too. However, I hated the dust from the MDF. I even had the local shop do most of the cuts - leaving only the final cuts and biscuits to me. I guess I won't know if the dust is harmful for 20 years - when I die from some carcinogen. Of course, after working with pressure treated lumber for years before they replaced it with stuff that was safe(r) - it's a toss up as to which will kill me first.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Architectural Millwork

  • KnowledgeBase: Architectural Millwork: Millwork Installer

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: Installation

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article