Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Machinery setup: Squaring up your saw       How to make sure your saw is cutting square. February 12, 2001

by Dan Rudusinovich

One of the most common questions my customers ask is: "How do we make sure that our saw is cutting square?" In this article, I'll explain the easiest way I've found to verify that your saw is cutting correctly. My methods apply to sliding table saws, vertical panel saws, table saws using miter gauges, and others.

When the fence is perpendicular to the blade I use a "five way cut method" to check the accuracy of my saw when the material is transferred through the blade at a 90 degree angle. This method can be used with a miter gauge on a table saw, a sliding panel saw, or a vertical panel saw when the blade travels through the material and the fence is stationary.

Start with a piece of material about 4 foot square and at least 5/8" thick (to give the test piece some stability). In a clockwise rotation, consecutively number each of the edges.

Start with the right hand edge at #1, then the bottom with #2, left hand edge with #3, the top with #4, and the right hand edge again with the number #5. Below, I've listed the steps required to check the accuracy of your saw. Be sure to rotate the test piece in a clockwise direction.

Step 1: With the #4 edge against the crosscut fence, cut off an 1/8" or more from edge #1. Then rotate edge #1 and place it against the crosscut fence.

Step 2: Cut off an 1/8" or more from edge #2, and then rotate edge #2 against the crosscut fence.

Step 3: With edge #2 against the fence, cut off an 1/8" or more from edge #3, and then rotate edge #3 against the fence.

Step 4: With edge #3 against the fence, remove an 1/8" or more from edge #4, and rotate edge #4 against the fence.

Step 5: With edge #4 against the fence, make a 2" cut on edge #5 and mark the top and the bottom of this cut. Now measure the top and the bottom. The difference of these two measurements divided by 4 will tell how accurate your crosscut fence is. This figure should not be greater than .004 of an inch.

When the fence is parallel with the blade, I use a 2-Way cut method to check the accuracy of a parallel fence (when ripping stock on a table saw, for example).

Start with a piece of 5/8" (or thicker) material about 4' square (or as large a piece as your saw will allow). Consecutively number all four edges.

Step 1: With the #2 edge against the fence, and feeding edge #1 into the saw first, cut at least 1/4" from edge #4.

Step 2: With the #4 edge against the fence, and feeding edge #1 into the saw first, cut at least 1/4" from edge #2.

Measure the width of the test piece at both ends, and divide any difference by two. The result will tell you how accurate your fence is.

Danny Radusinovich is Vice President of Buckner Weatherby Co. Inc.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Architectural Millwork: General

  • KnowledgeBase: Cabinetmaking: General

  • KnowledgeBase: Furniture: General

  • KnowledgeBase: Solid Wood Machining

  • KnowledgeBase: Solid Wood Machining: General

  • KnowledgeBase: Solid Wood Machining: Setup and Maintenance

  • KnowledgeBase: Woodworking Miscellaneous: Woodworking

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.