Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Making Acrylic Paint Stick Over Oil Paint       Quick answer: shellac primer. July 29, 2007

Question
We re-finish a lot of wood trim and cabinetry in San Francisco that is already oil based. It is convenient to re-finish in oil because, from our experience, oil sticks to oil so much better. We have walked into countless jobs where the previous paint job was latex over oil and coming off in sheets. We have converted many homes from oil to acrylic finishes, but only if we prime using great adhering water-based primers. When I ask companies about a semi-gloss acrylic that sticks to oil as good as a primer, they have few answers. Why is it so hard to find an acrylic finish enamel that will stick to oil as good as an $18 per gallon primer? Is there an industrial product out there that can be trusted to fit my needs?

Forum Responses
(Finishing Forum)
From contributor C:
Let me make sure I understand. You are refinishing cabs and trim that have previously been finished with a short or long oil alkyd pigmented finish, with fresh coats of the same. Is this after you've stripped and sanded the bulk of the old finish off, or are you just feathering the damages and filling and then applying fresh coats?



From the original questioner:
Sorry if I was unclear. In this scenario, we are not stripping the wood, merely re-painting wood trim, cabinetry, moulding, etc., that was previously finished with oil based pigmented paint. (In this case, not varnish, lacquer or any clear finishes.) That is why I'm interested in a water based enamel that will adhere to oil based enamel. While we have stripped entire homes of their wood finishes, this is not the common request of our clients, as it can be costly, of course. I should mention we spray as much as possible with a Kremlin Airmix and would like to continue to do so with any new product.


From contributor A:
When I do any kind of finish work and I don't know what the existing finish is, I spray or wipe on wb shellac. Shellac can be used as a binder coat for anything (I think). If you were going to put 2 coats of latex paint over the oil, you might be able to do 1 coat shellac and 1 coat latex.


From contributor C:
Your problem is not new or unusual. For decades I've used Zinnser bin primer, a shellac base pigmented primer that sticks extremely well to oil base or virtually anything else for that matter. After you have applied this, you may use any professional latex paint over the top of it.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: Refinishing




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article