Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Making Miter-Fold Corners with Wood Veneer       Detailed advice on tooling and techniques for making miter-fold countertops with wood veneer on an MDF substrate. August 21, 2006

Question
I want to make some miter fold tops out of 3/4"standard hardwood veneer on flake or MDF, similar to what the solid surface guys do. Does anyone have any recommendations on tooling or any tips on depth settings, etc?

Forum Responses
(CNC Forum)
From contributor A:
We have done quite a bit of miter fold work using wood veneer on a variety of substrates and find that MDF cores seem to machine and fold the best. We have used veneer core stock and depending on the core it can either fuzz up terribly or tear out. Feeds and speeds are dependant on the tooling and the job at hand. We have found that we had to experiment with depth settings to keep the fold line from breaking when using different veneers. When you get it set up it works slick. Most major tooling houses have inserted carbide blade cutters and the point is what goes the quickest. Most cutters are ground for a slight overbend to allow for glue so it sometimes becomes tricky to close and glue the miter to a true 90 without the use of an auxiliary block.



From contributor B:
This V Groove tool is a stock item. As mentioned, use an insert type router. As the point dwells in the cut the tip becomes dull first. This insert tool has 4 cutting edges, which can be used twice, reducing insert costs. Also, you have no diameter or Z axis changes, once insert is reversed. Most firms use a tape on the underside, then fold and glue.


From contributor C:
We use the attached picture on a horizontal aggregate.


Click here for full size image



From the original questioner:
I thought an aggregate may be the way to go but for only two tops I can't justify the cost.


From contributor D:
If you purchase the right aggregate, you will be able to use it for many other applications on your machine.


From contributor C:
We used to use a specially made saw blade and with a tip on it and a router bit that didn't have a point on it. We use a pod and rail machine so a router bit with a point pushes and one pass pushes the spoilage down and runs the fold so we always did 2 passes. You can use that aggregate for cove splashes on solid surface and we also run bead board with a set of cutters


From contributor E:
I use all of these methods and all will work, but if it is for a few tops why not use a table saw? You will get the best result this way. If not, the two pass method with the cone cutter will be the cheapest and about .005"-.01" from surface will work best (MDF preferred).


From contributor F:
I agree. In our shop we miter fold MDF core maple, cherry, oak all with excellent results just using a table saw. Someone mentioned taping the backside so if you are going to have to tape it anyway, why not go ahead and use the saw? It gives you a beautiful corner, lightly sandable and strong. We use a panel saw to rip the pieces to general size and to get perfectly straight cuts. For MDF it seems like about 97% of the time it will give you a 1-3 mm banana cut. We always straighten these out before putting the miter cut on them with the table saw.

It is tricky - use plenty of glue, but not so much that it opens your corner when folded (should squeeze out the back) and use blue tape so that the veneer doesn't peel out or fuzz up. We use tape across the joint about every 16 inches and then a long piece down the full length. We also tape taught all the way around the piece about every two feet to hold the angle at a 90. If you take your time when making the 45 you shouldn't have a problem getting a new perfect 90 when folded.

Make sure you don't get banana cuts when you cut the material or else when you cut the 45, you have the same banana cut, and then when you glue, same results. If you are having trouble getting the piece to line up when laid flat and the cuts butted up, then most likely you have a banana cut on one or both pieces. This will give you a piece with a bow in it. On short pieces it is not so much a problem but on 8 footers, it is a big problem. This is so much better than the way we used to make fillers and wrap around end panels.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Veneer

  • KnowledgeBase: Veneer: Techniques




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article