Does anyone know exactly what the difference is between marine plywood and interior plywood? Both use exterior grade glues on the substrates. My guess is the filler materials are different. If I build an outdoor bar and seal it will varnish, etc., won't they both hold up the same, since the finish will prevent water from entering the substrates?

Forum Responses
(Cabinetmaking Forum)
From contributor H:
Exterior grade is not the same as waterproof. I believe the glue used in marine grade ply is different. Another difference is the amount of void allowed in the cores of the plywood. Voids are where moisture can get trapped and are weak spots in the sheet. Marine plywood is made entirely of Douglas fir or western larch. Glue is completely waterproof. Grading of all plys is far better.

From Professor Gene Wengert, Sawing and Drying forum technical advisor
There are two adhesives, interior (which does not stand up to wetting) and exterior (which is not affected by long term wetting and would be called waterproof). Marine grade uses exterior adhesive, which is the same adhesive as used in the cheap CD-X plywood or any other exterior grade or "interior grade with exterior glue" plywood.

With marine grade, the lowest grade veneer is "B", which means that there will be no serious voids on the surface and interior plies. It is the voids that cause poor adhesion! So, marine grade will have good adhesion throughout the lamination. Also, marine grade can be cut without getting a void in one laminate on a freshly cut edge. The edges will be totally solid. The two species used for marine grade are Douglas fir and western larch, although I have seen keruing and other species used in a product called marine grade. You can get the same performance from panels such as exterior AC in most cases.

Marine grade has no natural decay resistance. It has no chemicals added to enhance decay resistance, unless it has been subsequently pressure treated (= $$$). Marine grade has no special waterproofing in or on the wood.

If you do not get the wood wet very often and if it is sealed, as you state, there is no difference in performance indeed by using a different, less expensive grade and species. Note that most interior grade panels do not use exterior adhesives. But if the plywood seldom gets wet, the interior adhesive will be just fine.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Lumber & Plywood: Buying

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article