Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Minimum Sticker Thickness       How thin can stickers be in order to maximize kiln capacity without creating drying problems? May 11, 2005

Question
Have there been any studies on what the minimum sticker thickness can be based on loading depth, fpm, moisture loss, operating temperature or rh%, etc? I want to maximize my kiln capacity without risking quality and/or productivity.

Forum Responses
(Sawing and Drying Forum)
From Gene Wengert, forum technical advisor:
What species and thickness? What initial MC in the kiln? I do recall a study that showed that 11/16" was the thinnest possible (in a specific situation). Most kilns are designed for 3/4", so that is what is used.



From contributor D:
I posted an earlier thread about sticker thickness. I made airflow sticks at 3/4" and they dried the first load of pine with no problems. You responded to a post about electric kilns and I'd like you to clarify the part about needing "1500kW or 150kw per day average". That didn't make sense. Is it watts and kilowatts? I am using electricity for heat in one kiln, and am unsure whether to hook it my boiler, being that htg oil is going to go through the roof. Perhaps this is the year to finally build that sawdust burning boiler.

The possibility of having degrade and uneven drying made the sticker thickness question easy for me... be a little conservative and avoid the problems.



From Gene Wengert, forum technical advisor:
1 kWh = 3,413 Btu = 1 kilowatt hour.


From contributor G:
I feel if you go under 3/4" stickers, you're pushing your luck. Seems like everyone is trying to push everything to the edge. I have a friend who has 17 80,000 bdft kilns, and they use 7/8" stickers. Their family has been in business for nearly 100 years. That told me all I needed to know.


From Gene Wengert, forum technical advisor:
With 7/8" stickers, compared to 3/4", you will reduce the kiln capacity by nearly 10% (which means you have more heat and venting per BF), you will increase the volume of air between the stickers (making drying more uniform), but will slow the overall air velocity (slowing drying at MC above 30% MC), and will increase air drying in a yard that is short on space and uses piles over 6' wide. With air dried lumber, there is no benefit in using thicker stickers and in fact, there are several production losses.


From contributor G:
Do you feel that 3/4" stickers are the best way to go? I do not air dry much, and when I do, it's only in the winter. Usually my lumber, mostly red oak, comes off the mill and goes directly into the kiln. I am running DH kilns. When I air dry during the warmer months I get too much degrade and poor color. Seem to get a lot of bug damage, also.


From Gene Wengert, forum technical advisor:
Yes. You probably can improve your air yard to avoid most damage.


From contributor L:
I am in the process of building my first solar kiln. Should the stickers be same height and width (3/4" x 3/4") or does width make a difference?


From Gene Wengert, forum technical advisor:
As 3/4 x 3/4 is fairly weak, many people will go with 3/4 x 1-14 or 1-1/2.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Lumber & Plywood: Storage

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Air Drying Lumber

  • KnowledgeBase: Primary Processing: General

  • KnowledgeBase: Primary Processing: Kiln Operation




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article