Today's
Sponsors:


Mereen-Johnson Machine Company

Merritt Woodwork

MFG in Honduras

Micro Fence

Microvellum

Middle Valley Lumber

Mikron Woodworking Machinery

Mill Outlet

Minimax

Mirror Reflections

MLS Machinery USA, Inc.

MLS Machinery

Modern Woodworking Magazine

Moldingknives.com

Monarch Machinery

Morbidelli

Moulder Services

Moulder Techniques

Mountainside Wood Products

Multicam, Inc.

NAP Gladu

Nebraska Tool

NEMI

New England Kiln Drying Association

NexGen

Hoffmann Machine Company

Holz Her U.S. Inc.

Howard S. Twichell Co.

Hvalsoe Sawmill Ltd.

ICA North America

Icy Straits Lumber

IDM

Impact Search and Placement

Indiana Hardwoods

Industrial Air Solutions

Integra Precision Grinding and Manufacturing

InTrading

Invicta Woodworking Machines

IpeDepot.com

irsauctions.com

Italpresse

J & G Machinery

J and J Barn Wood

J&P Machines

J. Gibson McIlvain Company

Jiffytops

JIT Hardware Supplies, Inc.

JMHsoftware.com

John G. Weber Co.

Joos USA Inc.

KCD Software

Kerber Farms and Mill

Keystone Wood Specialties

Keytrix Data Systems

Kiln-direct.com

Kleiberit Adhesives USA, Inc.

Kreg Tool Company

Kremlin

Lacy Cypress Inc.

Langelier Lumber Ltd.

Leadermac USA

Lewis Lumber Products

Lignomat

Logosol

Lumber Resources

Lumber Smith

M.L. Campbell

MACHINEKING.com

Macoser, Inc.

Mahros

Maine Timber Works

Maine Woods Company

Mann and Parker Lumber Co.

Martin Lumber

MARTIN Woodworking Machines Corp.

Mastercam - CNC Software

Matthews Mill

Maya Positioning Equipment




PVC for dust collection       Is it dangerous? April 2, 2002

Question
Is PVC drainpipe safe for ducting if I have it grounded, or should I go to the extra expense and use metal tubing?

Forum Responses
The main reason why PVC pipe is not recommended is the buildup of static electricity and the high risk of explosion.



Plastic pipe systems are not designed for dust collection use. A necessary diversity of fittings to meet design requirement does not exist. Also, plastic pipe elbows have a very short radius and plastic tee fittings are improper for dust removal. It is these types of problems that lead to an inefficient dust collection system.

With a metal dust collection piping system, static electrically won't develop. Elbows and other various fittings are properly designed for conveying dust. The diversity of fittings and accessories will enable you to meet design requirements.



I have found no problems using schedule 40 PVC. You do need to run a ground wire to each machine. As far as elbows are concerned, you can use electrical sweeps, which ease the bends. Also, don't use tees - use Y fittings.


I used plastic in my first shop. The static electric buildup was amazing. I tried to control it with ground wires, but still had problems. Don't take a chance on a dust explosion - use metal. Commercial heating contractors often stock the spiral duct and fittings since they are used in big buildings for air handling.


The National Fire Protection Agency recommends non-combustible ducting when conveying combustible material. As we know, wood dust is combustible, as well as PVC pipe, never mind the static buildup, which is a source of ignition.

When we create a duct system, the interior should be as obstruction-free as possible. A copper wire will snag chips and curls. In addition, many extraction systems are abrasive, such as the conveying of hardwood chips. This material will wear the copper wire.



When we had a PVC system in our shop, I had a chance to discuss the plastic pipe/static situation with an electrical engineer well-versed in industrial issues. According to him, there is virtually no way to protect a plastic based system. The static builds on the surfaces (inside or out) of the pipe and nothing but a continuous metallic ground (more like a coating than a wire) inside the pipe would mitigate the static buildup. He convinced me to get rid of the plastic and redo our system with metal pipe and fittings.

While removing the plastic (prior to a metal install) on a Monday after a non-working weekend, I noticed that the pipe still held a charge from the previous Friday's work. As a precaution I put on light duty rubber gloves. I got zapped right through the gloves by the static discharge from a length of pipe connected to the planer, which had been working hard the previous week. A few minutes later I picked up a piece of pipe that had also been connected to the planer and watched as a large spark arced from the pipe to my chest. These shocks were not life-threatening, as the discharge was mostly voltage with little amperage. That said, they made me painfully aware of the potential for static build-up.

You may get away with a plastic system for years, but some day when you are collecting large quantities of fine dust through your new wide-belt sander, disaster may strike. I'd never consider using anything but metal pipe for dust collection.



I have PVC in my shop and after a short while the static problem has gone completely away. I attribute this to dust/tracking within the system. It has worked out very well for me, is easily revamped into additional configurations as my shop has grown, and was readily available to me. I have no fear of an explosion ever occurring.


From contributor M:
Plastic pipe does indeed present a considerable risk. You may not have had any problems yet and you may know folks who have plastic systems that have not had problems. Simply because you have not had an explosion doesn’t mean that it can’t happen.

Though dust related explosions may not be an every day occurrence, they are not rare and the use of plastic pipe in a system that generates large amounts of fine flammable dust/particles is asking for a disaster.

I’ve seen first-hand evidence of what static discharge in dust collection systems can do. Practically speaking, it cannot be eliminated in plastic systems. When it discharges, it can ignite the dust in the system with explosive force. I’ve also spoken with experts in all phases of woodworking plant management and dust collection system design. They all condemn the use of plastic pipe and fittings for transport or collection of wood dust.



Dust explosions do occur in large commercial systems but there is a critical minimum size for an in cloud discharge. Lightning-like discharges in the dust cloud itself can ignite dust, but do not occur in dust clouds smaller than about 3 meters (10 ft) in diameter (Boschung, et al, p. 309).


From contributor M:
The reference you point to is clearly talking about the possibility of dust explosions in the “home shop”. We're not talking about home shops on this forum. The recommendations I've given and those from other industry experts are to avoid practices that can be dangerous.

I have personally experienced the dramatic effects of static discharge in pvc systems. I also have very reliable information of a dust system explosion, caused by static discharge, that caused a devastating fire in a commercial woodworking shop.

Frankly, I just don’t understand the zealous defense of pvc pipe dust systems. It’s potentially dangerous, and it’s only marginally cheaper and easier to install than standard metal pipe and fittings. I’m going to use pvc for plumbing and metal for dust system construction.



The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor A:
One of the biggest reasons that I will not have a PVC duct system is that I always jump when the static zaps me. The last thing I want when my hand is near a spinning cutter is a zap that may cause me to jump right into the cutter.



Comment from contributor R:
I had originally set up my small wood shop (14 x 20) with 3" PVC for my dust collection system because of the ease of working with the medium. I used the curved Y joints instead of 'T' joints eliminated any buildup in the bends as I routed it to the different machines. Plus being able to form and directly glue the blast gates to the pipe for a solid feel when opening was great.

Once I started reading all the adverse effects of the PVC in relation to static electricity I began to worry. As a test, I drilled the PVC pipe every 12" and screwed a 3/4" stainless sheet metal screw into the pipe and extending about 1/2' into the flow area. Each of these screws were then wired together and tied to the nearest electrical box for ground.

I haven't had any zaps while working with the system since. Again my shop is only 14 x 20 with 4 inputs to the 2hp system. Most of the collection is large particles from the table saw, router, combination saw and lathe. I use it to vacuum the floor as well.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Dust Collection, Safety, Plant Management

  • KnowledgeBase: Dust Collection, Safety, Plant Management: General

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article