Question
My customer wants to reface their black dishwasher with stainless steel to match their other appliances. I remember there is a company that sells a flexible self-stick metallic material that can transform the old looking appliances into the modern stainless look. Don't know who has this stuff. Any ideas? It's a KitchenAid dishwasher.

Forum Responses
(Cabinet and Millwork Installation Forum)
From contributor D:
The panels in Kichenaid are reversible - there are two color options standard on each one, and you can buy a replacement stainless panel top and bottom.



From contributor K:
Look at fauxstainlesssteel.com. I think this is the stuff you are talking about. I saw it used on an HGTV show. Alsa makes one in conjunction with GE. The other is ALKOR DECO, in Germany, but not sure if available in the US. Formica also makes a metal laminate in 96" x 40" sheets.


From the original questioner:
Thanks - exactly what I needed!

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: Installation


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2018 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article