Polyurethane Cure Times

      Polyurethane hardening times are temperature-dependent. With multiple coats, the process can get tricky. February 21, 2011

I'm putting down Minwax fast drying poly on an oak dining table, but after four days of drying the finish, it still feels rubbery. I could scratch into it if I tried. How long does it take to harden, or will it always be like this?

Forum Responses
(Finishing Forum)
From contributor R:
Did you also apply this fast drying poly over a Minwax stain? What's the temperature now and what was it when you applied the poly? Is the sample piece you made drier than the table, and did you finish this table the same way you completed your sample?

From the original questioner:
Yes, stain then Minwax polyshades, then fast drying poly. Temperature has been low, around 50 lately. No sample. Will high temperatures make the finish harder?

From contributor R:
From experience, it's very important to allow for correct drying times between each finishing step. If you apply too many oil based coatings on top of each other, and each of those coats has not properly cured, it's very possible that you will end up with a soft coating that may take weeks to dry.

Can you place the table in a dedicated room and crank up the heat? It's too late now, but it's always a grand idea to make a sample before doing the project. If Murphy wants to rear its ugly head, you're not so far into it if the sample goes boink. If the table hasn't fully cured by say Monday, you might have to strip it down and start over.

From the original questioner:
Thanks. I don't mind at all if it takes a month to cure, I just wanted to know if it ever would. I assumed it would be as hard after one day as it would be after a month, but maybe the cold weather isn't helping.

From contributor L:
Polyurethane takes 30 days to fully cure. It needs to be at about 70 degrees to cure properly within those 30 days. 50 degrees is pretty low and will retard curing fully within the 30 days.

From contributor D:
I'm just wondering why you put a fast dry poly over a slow dry poly (Polyshades)? This schedule seems destined for problems. If the Polyshade is not fully cured or at least dry, a fast drying product placed over it will cause problems - cracking of the underlying layers. This is how crackle effects are created. I would do as suggested - put in a heated area and hope for the best.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article