Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




Preventing Insect Infestation in Lumber Production       Pesticides have limited usefulness and significant hazards. Good yard hygeine and application of heat are the more practical choices. February 14, 2006

Question
I am cutting only softwoods - Western Hemlock, Douglas and Grand Fir, and maybe some Western Larch, into 1" boards. Do I need to worry about insect infestation? Should I spray it with Timbor, or something made for spraying on lumber products? I am stacking and stickering it to air dry, and will plane and edge it next year. Kilning is not an option. Any suggestions would be appreciated.

Forum Responses
(Sawing and Drying Forum)
From Dr. Gene Wengert, forum technical advisor:
Insect infestations are seldom a problem. Keep the yard area free of wood debris and you eliminate almost all the risk. Spraying the wood with an insecticide, even Timbor, only protects the outer layer of the wood, so any insects already inside are not controlled. Further, if you dry the wood aggressively, there is little risk. Of course, any insecticide you put on the wood will probably end up in the planer shavings and dust. Is this safe? Maybe you will wear a mask, wash your clothes and hands, etc., but maybe your customer will not. If you sell wood with an insecticide on it, do you need to legally provide the customer with a CIS and appropriate warnings? For many years (probably hundreds) commercial operations have not used insecticides for softwood lumber. Do you want to soak the wood in a product that will diffuse into the wood and so that the wood will contain this chemical for a long time?

Note that spraying the ground is only effective if the insects are out when you spray. Using a long-lasting insecticide is not safe, legal, environmentally responsible, or suggested. Always keep your lumber isolated from lumber sawn by someone else that may not be insect-free. This is especially true for any foreign lumber. There are fungicide and insecticide chemicals sold by several companies that are approved for lumber. They have a very short (30 days) life span, so they will safe when you get to processing the wood in a few months. However, if you are going to air dry for 6 months, you only have 1 month of protection and cannot reapply the products as they are all waterbased and you would be rewetting the wood.



From contributor A:
To Dr. Gene Wengert, forum technical advisor: Are logs for log homes that have been dipped in borate solutions safe to use, and does this process help to eliminate bug problems in the future? Could you give us some insight concerning commercial log home sales and proper treatment of the logs if any?


From Dr. Gene Wengert, forum technical advisor:
To contributor A: To be effective, borates must diffuse into the wood. This means that the borate solution (borates in water) must be in contact with the wood for a long time. Further, the wood must be fairly porous, so it would not work with white oak, heart maple, coastal Douglas-fir, wetwood hemlock, aspen, etc. A short dip will not allow the borates to penetrate into the wood deep enough and at a high enough concentration.

Borates remain water soluble, so that the logs, if they get rained on, will have the borates in these wet outer layers wash or leach out, and then provide no protection. Perhaps the best advice is to keep the logs dry, which means applying a water repellent finish to the outside and use appropriate construction techniques, including foundation ventilation, no shrubs against the walls, good roof overhang, etc.



From contributor B:
I'd recommend listening closely to what Dr. Wengert has to say on this. I needed short term protection for wood that I will be using myself and not selling. I have tried mint oil and pyretherins. Mint oil is the active ingredient in some sprays for ants and other bugs. I have bought it at some of the Big Box stores in aerosol cans. It smells good too. Pyretherins are harvested from flowers and break down in a matter of days to weeks depending on exposure to sunlight. Pyretherins can also make you sick so don't inhale it. There are synthetic versions of it too and the spelling is a little different. The synthetics are much stronger and don't break down as quickly and can make you really sick. The reason I mention this is that stores sell this stuff too for home use. The labels say they will kill PPBs and other wood boring insects. But remember, you are just treating the surface. The eggs are still in the wood and will hatch in the next year or two and then be in your home. Before you spray anything, just use the internet and search on a particular active ingredient before you treat anything, including your house. Some guys have had serious health problems from spraying things that they thought were safe.

My point is that you can find products that will deter wood boring insects without having to poison yourself. One idea I have is to try cedar oil but I'm not sure how well it will works or how to get it. Another idea that seems to be working is to surface the lumber. Some bugs like the rough surfaces and stay away from smooth surfaces. Believe it or not, it seems to be working. I have samples I am watching of boards cut from the same log lying next to each other. The bugs are going after rough one and leaving the other ones alone.

Anyone out there have anything they have tried? I'd like to know what worked and what didn’t work.



From contributor C:
I've applied a solution yearly of cedarwood oil and neem oil in a distilled turpentine vehicle to totem poles. While this doesn't scare off the carpenter bees, we have never been bothered by PPB or carpenter ants. It even keeps off the paper wasps which like to pull off fibers for their nests. Cedar oil is avail through many chemical companies. What you are getting is probably made in China and is an extract from a juniper, like our ERC or aromatic cedar. I've also used boric acid applied with water and a roller as a vain attempt to forestall green stain in holly. It didn't work on the stain fungus, but insects hate it so it would probably deter any egglayers. I think as far as the beetles are concerned, good housekeeping is the key, and you should also keep an eye on the wood and look for frass (the dust that piles up outside a grub hole). If you find them, blast them quick with heat.


From Dr. Gene Wengert, forum technical advisor:
The lyctic PPB only affects hardwoods and mainly the grainy hardwoods like oak and ash. Are your totems softwoods? If so, that is why you do not see the lyctid PPB.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Air Drying Lumber

  • KnowledgeBase: Primary Processing: Kiln Operation

  • KnowledgeBase: Primary Processing: Sawmilling




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article