Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Quality of Southern Grown Oak       Though slightly different from northern wood, it's suitable for furniture. July 12, 2005

Question
I am interested in finding out if white and red oak grown in the south (midwest GA) are suitable for constructing fine furniture. I have been told that due to the longer growing season in the south, the growth rings are not as tight as those grown in colder climates. Does this have an effect on the quality of the wood?

Forum Responses
(Sawing and Drying Forum)
From contributor E:
I live in south AL and have been using red and white oak for years in my shop. I've made just about any kind of furniture out of each, and have not had any problem with either. I also custom saw both for other people.



From contributor B:
I run full time near Andalusia in south AL, and cut, sell, and even use quite a bit of red and white oak. It sells fine for small shops - even cabinet shops love it kiln-dried. The problem I've run into is moving it in quantity to larger millwork shops. I guess it depends on the area in which you are selling and what they think fine furniture might be.


From contributor C:
Maybe someone can correct me if I am wrong, but I was not aware that tightness of growth rings was important in ring porous hard wood. Many times I have read that new growth hard wood (wider growth ring) is stronger than old growth hard wood (narrower growth ring). Also, the appearance in furniture of either is in the eye of the beholder.


From contributor L:
Southern oak is fine for furniture if it's dried to correct moisture content. If the moisture content varies by more then 2%, the southern oak will be more prone to splitting or joints opening since they are more dense and will move more then a northern wood. Just make sure it's dried to the correct moisture content with adequate moisture tolerances.


From contributor G:
Southern hardwoods are fine unless you are used to northern (especially oak). Here, southern red oak is referred to as Appalachian oak and interpreted as being available in long and clear lengths, but not as desirable or stable as northern red. The southern will work just as well and nobody but those with trained eyes will know or care about the difference. If you mix the two, a difference in color and texture will show an undesirable difference.


From Gene Wengert, forum technical advisor:
Southern oak has a lot more sapwood than northern or Appalachian. As the sapwood stains (fungal and chemical grey stain) easily, this means some loss of color in a few pieces. The rings are spaced further apart in southern, but this means slightly stronger wood. The color is often more red, especially in cherry bark (or southern red) oak. Often southern air drying is more rapid than northern, leading to more checking risk in the south. Southern white oak (lowland) does seem to check quite a bit more easily than other oak even at the same RH conditions.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Primary Processing: General

  • KnowledgeBase: Wood Engineering

  • KnowledgeBase: Wood Engineering: Wood Properties




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article