Today's
Sponsors:


BetterVacuumcups.com

Biesse America

Biewer Lumber

Binks

Black Bros. Co.

Blackhawk Machinery

Briquetting Solutions by Sunomi LLC

Brown Wood Products Co.

Business Management Solutions

Byrd Tool

C.R. Onsrud

Cab Parts

Cabinet Door Service Co.

Cabinet Pro

CabinetCRUNCHER Cutlist & 3D Cabinet Design Software

Cabinetmakers Association

CADCABINETS.COM

CADCode

Cag Lumber

Cantek America

Carolina Woodworking Consultants

Carter Products

Carving Technologies

Castle

Catskill Timber Industries

Charles G.G. Schmidt Co.

Chicago Dowel Company, Inc.

Clear Lake Lumber

CNC Parts Dept.

1-800-Cabinets.com

2Sand.com

3M Corporation

A O M Spray Equipment

Abrasive Resource

Accu-Router, Inc.

AceCo Precision Wood Tooling

Activa

Air Handling Systems

Alan McIlvain Company

Algoma Lumber Co.

All Star Adhesives

Alliance Millsoft

Allied Machinery Inc.

AllRout

Amana Tool

Ameitech South

American Fabric Filter Co.

American Institute of Building Design

American National Woodworking Knife

American Rotary Converters

Andreou Machinery

ANEST IWATA USA, Inc.

Antique Beams and Boards

Antique Building Materials

Anver Corporation

Apollo Sprayers Inc.

Arbor Processing Inc.

Architectural Elements

ArtCam

ATEMAG

Atlantic Machinery Corp.

Auton Motorized Systems

AWFS

B.H. Davis Company

Bailey's Inc.

Baker Products

Banks Hardwoods

Barn Detail

Barn Door Lumber

BC Wood Specialties Group

BeamsRUS

Beaver Tools

Benz Incorporated

Best Cabinets




Scratch Marks from Hand Sanding       Basic advice on appropriate hand sanding technique to minimize visible scratch marks. December 29, 2008

Question
How do you get sander marks out of wood before staining?

Forum Responses
(Finishing Forum)
From contributor M:
Don't know if you're referring to hand sanding or large production sanders, but the method is pretty much the same. I usually start with 100/120 grit and work my way through each successive grit (100, 120, 150, 180, 220) up to about 180 grit. Usually when you go above 180 you begin to compromise the ability of the stain to penetrate the wood. Good way to check for sanding marks before staining is to wipe the wood with lacquer thinner or mineral spirits and view with a high angle light source.



From the original questioner:
Thank you very much. Is it still okay to go back and use different grits after you have already tried 220? And they are production sander marks.


From contributor M:
Shouldn't be a problem unless you are working with thin veneer (1/32") on a substrate. Each successive grit removes the scratches from the previous grit and leaves a finer scratch pattern which is then removed by the next finer grit sanding... and so on and so on.

So yes, as long as you don't think there is any danger of sanding through, you should be able to start over again with no problems.

Is this on a wide belt Timesaver type machine? What type of material are you sanding? What type of finish are you using? Could probably give you a little better direction with answers to these questions.



From the original questioner:
Thank you. Actually, it was a 1/3 sheet sander. Not sure if it was the right tool to work with. I am working with oak. I am looking to use a stain from Zahr to finish it.


From contributor S:
1/3 sheet sander is fine. Pigment stain doesn't penetrate the wood exactly the way a dye would, but the pigment hangs up in the grain and sanding scratches, hence the reason for minimizing them as much as possible.

When using a 1/3 sheet (or 1/4) vs. an orbital sander, there is an easy way to know that you have removed all the previous grits scratches. It does go against logic and the usual teaching and you have to pay attention to being thorough. You will be alternately sanding with the grain and against the grain of the wood.

Decide what is the final grit you are going to sand to and that grit will be sanded with the grain of the wood. If you want to sand to 220 and you are starting with 120, 150, 180 then your sanding schedule would begin by sanding against the grain with the 120. With the grain with 150, against the grain with 180, and with the grain for your final 220.

This makes it very clear and easy to know when you have removed all of the previous scratches. It is important to change your paper frequently especially on the finer grits, and make sure you do not allow junk to build up on the paper, which can leave deeper scratches.

It should take just about half the amount the sanding time on successive grits (to remove the previous) as it took for the previous coarser grit, but again, keep your paper fresh. One of the toughest points I ever have had to get across in training others is that their labor involved in overuse of a piece of sandpaper far outweighs the cost of the sandpaper, not to mention it simply stops being effective when overused. Try it on a sample first and see if it works for you.



From contributor G:
Depending on the wood, you can get away from a lot of sanding by hot water-popping the wood, which will swell up the fibers and raise out the swirls. After it dries, you can sand with the grain and get rid of them all with 180.


From contributor N:
A good high-speed orbital sander shouldn't leave sanding marks visible to stain even at 120 grit. It is not necessary to have a five-step sanding process to eliminate scratches.


From contributor G:
Use an inspection light properly and you can see all sanding marks plainly, even sanding marks you don't need to see and won't show. Nothing special about the lights - a car headlamp will work. You need it bright. The light should be at a very low angle across the top, shining across it, not down. You'll know when you get the proper angle - all the details in the top will jump right out.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article