Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Scribing loose end panels       Woodworkers describe the processes they use. April 3, 2002

Question
It seems that scribing is one of the tougher concepts to teach rookies. I thought I'd describe how I scribe loose end panels (this particular example was for a high-end installation). Hopefully, this post will shed some light on the general scribing process as well as a "loose panel" scenario.

First, I clamp the loose end panel in place, and check the reveal at both the top and bottom. The cabinet is typically hung plumb, but in the event that it's a tad out of plumb, relying on the reveal will ensure that the fit matches the cabinet. I clamp the panel just loose enough so I can bump the panel to adjust the reveal. When the reveal is equal top and bottom, I tighten the clamp.

Next, I set my scribe to the distance shown in the sketch below:

Then I mark the cut line on the end panel.

Next, I cut as close to the line as practical, with the saw set at a 30 degree bevel.

The bevel (shown below) allows me to fine-tune the cut using a block plane. If I had made a square cut, I'd be removing the full 3/4" as I adjusted the cut to match the line. This bevel also allows me to cut the panel 1/16th or so heavy, and I loosen the cabinet a bit, install the panel, and then draw the cabinet tight to the wall. The sharp beveled edge will actually "cut" itself into the drywall for a fit that can't be beat.

Forum Responses
From contributor L:
I don't use a belt sander to scribe (used to several years ago). If it's a loose panel, I will rip it within 1/8 of where it needs to be, then by holding or clamping it in place (depending), I scribe it and sand it with a grinder and finish it with a file.

This system works well for me as I have mastered the art of using a grinder. I even use it on p-lam top deck seams. Most carpenters use a belt sander to scribe and are reluctant to try using a grinder. I was one of them, but now I would never go back to using a belt sander for scribe work. Sanding disks are less expensive and grinders are small - easy to stuff into your bat box. Ergonomics is an important factor as well as increased speed and overall flexibility.



From contributor R:
The first time I was asked to use a grinder I thought the idea was a joke. I am a better cabinetmaker than that - "I use a router". Turns out that the grinder is easier, faster and doesn't chip at the end of a cross grain cut. You can almost scribe the end of a countertop like a hot knife through butter. I have a 4" DeWalt and what I like about it is the shaft lock - you can change disks without any tools.


From contributor M:
I've got several grinders laying around that I bought at auction but never thought of using them in the woodshop. What type of wheel are you using? The stone disk used for removing paint and cleaning up before welding?


From contributor M:
I have used most grinders and the one I like best is the DeWalt, specifically the DW402 4 1/2" angle grinder. DeWalt makes a sanding disk attachment specifically for the DW402. I use 36 grit disks with it for fast stock removal. If you can deal with the learning curve you will see a 100 to 200+% increase in speed on scribe work.


From contributor B:
I use an offset router with a wheel centered on the router bit to follow the wall and do the cutting for me. I use it for cabinet ends, panels and tops mostly. First I level and plumb the cabinets. Next I set the panel or end or top 1" from the wall to where I want the cut to be made, clamp or screw it in place temporarily, and run the router from right to left along the wall. If I go the wrong direction, the router wants to pull into the piece I am scribing and that causes problems.

It cuts a clean line that fits like a glove. And you can usually do two adjacent walls in a corner or wall and ceiling at the same time. I also do plunge cuts with it where I need to get around outlets or whatever. Just hold the wheel against the wall and rock it in or out.

Solid stock tends to want to split along the grain, so I make a shallow cut with the router and jigsaw off the rest.

This is faster, easier and does a better job than anything I have seen, be it sanders or saws or grinders or planes. You can throw away your compass, too, since it makes the cut, not just a line to cut to. The only thing is you need to be able to pull the piece away from the wall 1" to make it work.



From contributor M:
Sanding attachment... okay. I brought my Dewalt 4 1/2 angle grinder yesterday with the grinding stone, and it didn't work so well. Lots of smoke!


From contributor R:
You need to get the right paper for sanding. I get mine at a welding supply store. They have from 36 grit to 120 grit. Use the back-up pad that came with the sanding attachment, which you need to purchase separately. There should be no smoke.


To the original questioner:
1. When you set up for your loose panel scribe, do you aim to get equal widths on the scribed rail as on the outer loose panel rail or do you aim to get an equal width with the sum of the (outer rail + edge of face frame)?

2. When your back scribe is complete, do you flush up the extended edge of the face frame with the outer face of the front stile of the loose panel?

3. Do you V-groove this butt joint formed by the extended edge of face frame and the loose panel?

4. In your next to last photo you seem to be cutting along a straight edge. Usually a scribe is less than straight. Are you rough cutting a straight line and then planing to your scribe line?

Contributor B, what type of offset router are you talking about? Type and size of bit? I don't see how your method could work for the end panel scribe that the questioner is showing in the photos. Could you describe a little more about how you would do it?



From the original questioner:
1. I think you mean stile here instead of rail... the end panels are made with an oversize stile on the scribe side (typically 1" wider). If the panel was made 1" over size, and no extra material was added to the scribe stile, removing 3/4" of the scribe rail would make a "weak" looking stile. My experience (and eye) finds that a "heavy" stile is far less noticeable then a "weak" one. I make no cut on the face frame side of the panel - only the scribe stile gets whacked.

2. The face frame extends an inch beyond the plywood cabinet side, resulting in a 1/4" reveal after the panel is installed. The 1/4" reveal is very forgiving in the field (as opposed to trying to flush this spot up). Here's a sketch of this detail:

3. The panel edge is slightly eased when it's made, which again makes this spot much more forgiving during the install. The easing isn't a must, but a nice touch.

4. You got it - I cut as close to the scribe line as possible with the straightedge, and then shave the remainder with a *sharp* block plane. There's been a lot of mention about using a grinder or belt sander, and while they may make sense for laminate backsplash scribes and other "heavy" scribes, a block plane is my tool of choice in this situation. It fits in my pouch, doesn't require safety glasses, is quiet, and most importantly, allows me to fine tune the scribe with one hand while I support the panel with my other hand (which all adds up to *faster*, in case you think I'm sounding like a purist). It's also a lot harder to ruin a panel with a block plane then a grinder or sander... I think most installers don't consider using a block plane 'cause they haven't broken the learning curve of sharpening one. When they're razor sharp (literally), they're awesome tools. When they're not razor sharp, they might as well stay home.



From contributor B:
The router I use is a Bosch #1609 with the offset base. It has a Quickscribe attached to the bottom, which is a wheel centered on the bit that follows the wall and guides the router.

I use a sharp 1/4" straight carbide cutter projecting 1/4" to 3/8" out from the router base. It will cut more, but I rabbet cabinet ends, etc. so I don't have so much to cut. It is also easier on the tool that way. I don't like to abuse my tools, although the price of a router is still cheap when I consider the time (money) I save.

To scribe the end the questioner is doing, I would screw a 1" spacer to the cabinet end 2" out from the wall to get it parallel with the cabinet end, then use 2 clamps to secure the end to the cabinet with the outside edge 1" out from the back of the face frame. Assuming the face frame is 3/4" thick, the panel edge would be out 1/4" from the face of the cabinet. It is 1" from the wall to where the router cuts.

Next I would run the router up the panel, holding the wheel against the wall, making a 1/4" or so deep cut. Solid wood tends to split if I try to cut all the way through with the router. If I were to go the other direction, the router might pull into the panel and cut too much.

Unclamp the panel and finish the cut with a jigsaw, using the cut made with the router as your line. I bevel that cut a little except at the bottom where you would see it. This cut doesn't have to be neat because you don't see it. Remove the spacer and put the panel in place.

It might work without the 1" filler, but the edge of the wheel may leave a mark on the wall because of the angle created by the face frame being out 1" from the end. The wheel has a chamfer on the edges, but it is probably best to use the flat part of the wheel against the wall.

I agree on the sharp block plane for times when the router won't work. I have much more control over what I am taking off than with a belt sander, plus it is faster than having to clamp the panel down someplace to use a sander or grinder. I really like my Bosch jigsaw for rough cutting before using the block plane.

The Quickscribe is a new tool I got that cuts my scribing time way down. An average 8' plastic laminate top takes less than 5 minutes to scribe and the fit is unbelievable. The more I use it, the more uses I find for it.



I think what's becoming evident here is that the real issue is: "Are they face-framed cabinets or are they Euro-style cabinets?"

My experience, for all practical matters, is solely face frame. Using a block plane with laminate/composite panels doesn't seem to make much sense. Both styles have their merits. I still think the reason the block plane has fallen out of favor (for all you face frame installers) is because no one knows how to sharpen the things anymore.



From contributor L:
If I were installing real wood, I would enjoy my block plane. But the only real wood I come in contact with these days is 4mm thick embodied with MDF, particle board or fire treated, so in my case a grinder, electric planer or router is preferable.


I do mostly Euro cabinets with probably 60% being plastic lam faces, the rest wood. The block plane works great for both wood and laminate as long as it is sharp. I wouldn't be without it.


What I have used and seems to be standard around here on high-end stuff is end panels that have 1/2" added to width of scribed stile (or whatever part), the back of that edge rabbeted 1/2x3/4 (on 3/4 material). The installer sets the piece plumb and level and scribes with tape and knife and 1/2" block, removing the outside piece of tape left. Then jigsaw or power plane, angled, outside the line left at the tape edge and clean up with a sanding block, belt sander, file or whatever suits.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Architectural Millwork

  • KnowledgeBase: Architectural Millwork: Millwork Installer

  • KnowledgeBase: Business: Project Management

  • KnowledgeBase: Cabinetmaking: Installation

  • KnowledgeBase: Woodworking Miscellaneous

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801